Yakela-Dalaoba Gas Well Downhole Tubing Corrosion and Protection Measures
摘 要
雅克拉-大涝坝凝析气田投产5年时间内, 因腐蚀报废油管15500 m。通过对气井腐蚀环境、井下油管腐蚀状况和失效状况进行分析, 根据结论提出采用有利于腐蚀防护的先进完井工艺, 采用升级管材和特殊扣型的扣内涂层管, 探索改性金属油管的使用和采用阴极保护等腐蚀防护措施和建议。
Abstract
Yakela-Dalaoba gas condensate field locates in Xinjiang Tarim Basin. The reservoir property belongs to high depth (5000-6000 m), high pressure (56-58 MPa), high temperature (146-150 ℃) and complex corrosion environment (high CO2, high Cl-, low pH , low H2S ). After the field was put into operation for 5 years, due to the occurrence of corrosion of underground pipes 15, 500 meters tubing were scrapped. After analyzing the Yakela-Dalaoba corrosive environment and the failure in hole tubing, the gas well downhole tubing corrosion protection measures and recommendations are proposed.
中图分类号 TG172.8
所属栏目 应用技术
基金项目
收稿日期 2011/1/26
修改稿日期 2011/2/7
网络出版日期
作者单位点击查看
备注杨刚, 助理工程师,
引用该论文: YANG GANG,LIANG Gen-sheng,CAI HONG. Yakela-Dalaoba Gas Well Downhole Tubing Corrosion and Protection Measures[J]. Corrosion & Protection, 2011, 32(12): 1001
被引情况:
【1】乔学华, "雅克拉井下油管结垢腐蚀分析及防治措施",腐蚀与防护 34, 957-959(2013)
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】余一刚. 雅克拉油气集输管材及内层涂料选用研究评价[J]. 油气田地面工程, 2004, 24(5): 107-110.
【2】李慧, 黄本生. 陶瓷复膜抗腐蚀技术在井下工具防腐中的应用[J]. 天然气工业, 2008, 28(4): 114-116.
【3】翁永基. 材料腐蚀通论-腐蚀科学与工程基础[M]. 北京:石油工业出版社, 2004:230-232.
【2】李慧, 黄本生. 陶瓷复膜抗腐蚀技术在井下工具防腐中的应用[J]. 天然气工业, 2008, 28(4): 114-116.
【3】翁永基. 材料腐蚀通论-腐蚀科学与工程基础[M]. 北京:石油工业出版社, 2004:230-232.
相关信息