Synthesis and Inhibition Performance of Quaternary Ammonium Salt Gemini Surfactant
摘 要
以邻苯二甲酸为连接基,油酸酰胺为主体,氯化苄为成盐试剂,合成了一种新型的季铵盐双子型表面活性剂(ODOB)。它具有更多的吸附基团,水溶性良好。SEM结果显示,其在钢片表面具有很好的吸附成膜性能,能在碳钢表面形成单分子的吸附层,一个缓蚀剂分子可以取代2.7个水分子。电化学和失重法结果显示,ODOB通过增大反应的活化能来抑制腐蚀速率,其质量浓度为150 mg/L时,在10%的盐酸(25 ℃)中的缓蚀率可以达到99.3%。
Abstract
A new kind of quaternary ammonium salt gemini surfactant(ODOB) was synthesized by oleic amide, phthalic acid and benzyl chloride which were used as main body, bonding group and salt reagent respectively. ODOB has more adsorption groups and good solubility in water. The results of SEM show that ODOB has good adsorption film performance on the steel surface. ODOB can form a single molecule adsorbed layer, and a corrosion inhibitor molecule can replace 2.7 molecules of water. The results of electrochemical test and weight loss method show that ODOB can inhibit the corrosion rate by increasing reaction activation energy, the corrosion inhibition rate was up to 99.3% when its concentration was 150 mg/L.
中图分类号 TG174.42
所属栏目 试验研究
基金项目 国家科技重大专项(2011ZX05026-004-04)
收稿日期 2013/1/5
修改稿日期
网络出版日期
作者单位点击查看
备注叶天旭(1973-),副教授,博士,从事精细化工等新材料的开发,
引用该论文: LI Meng,YUE Wei-chao,XU Ji-zhan,YE Tian-xu. Synthesis and Inhibition Performance of Quaternary Ammonium Salt Gemini Surfactant[J]. Corrosion & Protection, 2013, 34(12): 1058
被引情况:
【1】余祖孝,郝世雄, "Na2MoO4对AZ61镁合金电化学行为的影响",机械工程材料 39, 56-59(2015)
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】刘福国. 油田钻具、管道系统腐蚀规律及缓蚀剂缓蚀性能和机制研究[D]. 青岛:中国海洋大学硕士学位论文,2008.
【2】段永锋,于凤昌,崔新安. 缓蚀剂在油气田集输系统的应用与研究进展[J]. 石油与天然气,2010,24(6): 26-30.
【3】李强,熊金平,左禹,等. Gemini表面活性剂的缓蚀性研究[J]. 石油化工腐蚀与防护,2011,28(1):9-13.
【4】EIAWADY A A,ABDEINABEY B A,AZIZ S G. Kineticthermodynamic and adsorption isotherms analyses for the inhibition of the acid corrosion of steely cyclic and open-chain amines[J]. J Electrochem Soc,1992,139(8):2149-2154.
【5】AAHASSI Sorkhabi H,MAJIDI M R,SEYYEDI K. Investigation of inhibition effect of some amino acids againststeel corrosion in HCl solution[J]. Applied Surface Science,2004,225(4):176-185.
【2】段永锋,于凤昌,崔新安. 缓蚀剂在油气田集输系统的应用与研究进展[J]. 石油与天然气,2010,24(6): 26-30.
【3】李强,熊金平,左禹,等. Gemini表面活性剂的缓蚀性研究[J]. 石油化工腐蚀与防护,2011,28(1):9-13.
【4】EIAWADY A A,ABDEINABEY B A,AZIZ S G. Kineticthermodynamic and adsorption isotherms analyses for the inhibition of the acid corrosion of steely cyclic and open-chain amines[J]. J Electrochem Soc,1992,139(8):2149-2154.
【5】AAHASSI Sorkhabi H,MAJIDI M R,SEYYEDI K. Investigation of inhibition effect of some amino acids againststeel corrosion in HCl solution[J]. Applied Surface Science,2004,225(4):176-185.
相关信息