Oxide Dispersion Strengthening Nickel-Based Superalloy Prepared by Supersolidus Liquid Phase Sintering
摘 要
采用超固相线液相烧结法制备了纳米Y2O3质量分数为0~8%的氧化物弥散强化镍基高温合金, 研究了烧结温度、Y2O3含量对该合金组织和力学性能的影响。结果表明: 含1.5% Y2O3的合金经过1 265 ℃真空烧结2 h后, 综合性能最佳, 相对密度为98.13%, 抗拉强度为770 MPa, 后续的热等静压处理可以促进合金的致密化, 使抗拉强度进一步提高, 达838 MPa。
Abstract
Oxide dispersion strengthening(ODS) nickel-based superalloys with different contents of nano Y2O3 (0-8wt%) were prepared by supersolidus liquid phase sintering method. The effects of sintering temperature and Y2O3 content on the microstructure and mechanical properties of the alloy were studied. The results show that the alloy with 1.5wt% Y2O3 sintered at 1 265 ℃ for 2 h had optimal comprehensive properties, that the relative density was 98.13%, tensile strength was 770 MPa. The relative density of the alloy could be improved further by following hot isostatic pressing process, tensile strength could be increased to 838 MPa.
中图分类号 TF125.5
所属栏目
基金项目 高等学校博士学科点专项科研基金项目(20080480032)
收稿日期 2010/7/6
修改稿日期 2011/2/7
网络出版日期
作者单位点击查看
备注李俊(1984-), 男, 湖南娄底人, 硕士研究生。
引用该论文: LI Jun,XIONG Wei-hao,YANG Qing-qing,LI Xiao-feng. Oxide Dispersion Strengthening Nickel-Based Superalloy Prepared by Supersolidus Liquid Phase Sintering[J]. Materials for mechancial engineering, 2011, 35(9): 85~88
李俊,熊惟皓,杨青青,李小峰. 超固相线液相烧结制备氧化物弥散强化镍基高温合金[J]. 机械工程材料, 2011, 35(9): 85~88
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】PARK L J, RYU H J, HONG S H, et al. Microstructure and mechanical behavior of mechanically alloyed ODS Ni-base superalloy for aerospace gas turbine application[J]. Advanced Performance Materials,1998,5:279-290.
【2】INOUE T, TANAKA K, ADACHI H, et al. Evolution of orientation distributions of γ and γ′ phases during creep deformation of Ni-base single crystal superalloys[J]. Acta Materialia,2009,57(4):1078-1085.
【3】郭建亭. 高温合金材料学[M]. 北京:科学出版社,2008.
【4】孔祥鑫. 第四代战斗机及其动力装置[J].航空科学技术,1994(5):21-23.
【5】周瑞发. 高温结构材料[M].北京:国防工业出版社,2006.
【6】BENJAMIN J S. Dispersion-strengthened superalloys by mechanical alloying[J]. Metallurgy Transactions,1970,1(10):2943-2951.
【7】BENN R C, BENJAMIN J S. Nickel-based dispersion-strengthened alloys[J]. Mechanical Properties of Metallic Composites,1994,7:319-339.
【8】GERMAN R M.Supersolidus liquid-phase sintering of prealloyed powders[J]. Metallurgical and Materials Transactions A,1997,28:1553-1567.
【9】LAL A, IACOCCA R G, GERMAN R M. Densification during the supersolidus liquid-phase sintering of nickel-based prealloyed powder mixtures[J]. Metallurgical and Materials Transactions A,1999,30:2201-2208.
【10】曾德麟,张怀泉. 超固相液相烧结[J].粉末冶金工业,1995,25(1):6-11.
【11】吴卫东, 柳光祖, 李华林, 等. 氧化物弥散相的分布对ODS镍基合金高温持久性能的影响[J].材料工程,1996(8):6-9.
【12】汤春峰, 曲选辉, 王天剑, 等. 超固相液相烧结GH4049粉末合金[J].粉末冶金技术,2007,25(2):104-108.
【13】黄培云. 粉末冶金原理[M].北京:冶金工业出版社,1997.
【14】符夷雄, 杨敏. 热等静压对硬质合金强度的影响[J].地球科学-中国地质大学学报,1996,21(6):645-646.
【2】INOUE T, TANAKA K, ADACHI H, et al. Evolution of orientation distributions of γ and γ′ phases during creep deformation of Ni-base single crystal superalloys[J]. Acta Materialia,2009,57(4):1078-1085.
【3】郭建亭. 高温合金材料学[M]. 北京:科学出版社,2008.
【4】孔祥鑫. 第四代战斗机及其动力装置[J].航空科学技术,1994(5):21-23.
【5】周瑞发. 高温结构材料[M].北京:国防工业出版社,2006.
【6】BENJAMIN J S. Dispersion-strengthened superalloys by mechanical alloying[J]. Metallurgy Transactions,1970,1(10):2943-2951.
【7】BENN R C, BENJAMIN J S. Nickel-based dispersion-strengthened alloys[J]. Mechanical Properties of Metallic Composites,1994,7:319-339.
【8】GERMAN R M.Supersolidus liquid-phase sintering of prealloyed powders[J]. Metallurgical and Materials Transactions A,1997,28:1553-1567.
【9】LAL A, IACOCCA R G, GERMAN R M. Densification during the supersolidus liquid-phase sintering of nickel-based prealloyed powder mixtures[J]. Metallurgical and Materials Transactions A,1999,30:2201-2208.
【10】曾德麟,张怀泉. 超固相液相烧结[J].粉末冶金工业,1995,25(1):6-11.
【11】吴卫东, 柳光祖, 李华林, 等. 氧化物弥散相的分布对ODS镍基合金高温持久性能的影响[J].材料工程,1996(8):6-9.
【12】汤春峰, 曲选辉, 王天剑, 等. 超固相液相烧结GH4049粉末合金[J].粉末冶金技术,2007,25(2):104-108.
【13】黄培云. 粉末冶金原理[M].北京:冶金工业出版社,1997.
【14】符夷雄, 杨敏. 热等静压对硬质合金强度的影响[J].地球科学-中国地质大学学报,1996,21(6):645-646.
相关信息