The Reliability and Progress of Life prediction Methods for High Temperature Pressure Pipes in Thermal Power Plants
摘 要
综述了当前常用的几种火电厂高温压力管道寿命预测的方法及模型, 包括持久强度法、时间参数外推法、θ法与修正的θ法、蠕变曲线外推法和蠕变损伤法, 深入讨论了各方法适用条件和可靠性。最后, 对与高温压力管道寿命预测有关的几个技术问题进行了分析和展望。
Abstract
Several current life prediction methods and models for high temperature pressure pipes in thermal power plants were introduced, including persistent strength method, time parameter exptrapolation method,θ method and θ method of amendment, gradual extrapolation method based on creep curves and creep damage method. The reliability of these methods was deeply discussed. Then application conditions and brief commentaries to these methods were given. Finally, several technical problems about life prediction of the high temperature pressure pipes were analyzed and predicted.
中图分类号 TM621
所属栏目 综述
基金项目 浙江省科技厅重大科技专项资助项目(2010C11068); 浙江省自然科学基金资助项目(Y1091078)
收稿日期 2011/12/22
修改稿日期 2012/8/16
网络出版日期
作者单位点击查看
备注蔡庆木(1987-), 男, 浙江温州人, 硕士研究生。
引用该论文: CAI Qing-mu,LIU Yue-ming,HUANG Chang-qing,LOU jun,TIAN Wei-jian. The Reliability and Progress of Life prediction Methods for High Temperature Pressure Pipes in Thermal Power Plants[J]. Materials for mechancial engineering, 2012, 36(12): 5~9
蔡庆木,刘月明,黄昌清,楼俊,田维坚. 火电厂高温压力管道寿命预测模型的可靠性及进展[J]. 机械工程材料, 2012, 36(12): 5~9
被引情况:
【1】江冯,刘春慧,程从前,赵杰, "采用不同方法预测10Cr9MoW2VNbBN钢蠕变曲线的比较",机械工程材料 39, 89-93(2015)
【2】黄维浩,张瑞,唐松青,赵中平,彭行金, "运行15 万h后F12钢主蒸汽管道剩余寿命的预测与试验验证",机械工程材料 38, 90-95(2014)
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】李益民,束国刚,梁昌乾.电站高温部件蠕变寿命预测方法[J].热力发电, 1994(2):38-44.
【2】扬宜科, 吴天禄, 江先美, 等. 金属高温强度及试验[M].上海: 上海科学技术出版社, 1986.
【3】EVANS R W, WILSHIRE B. Creep of metals and alloys [M].US IMM North Americen Pub,1985.
【4】束国刚,李益民,赵彦芬, 等.基于蠕变曲线的12CrlMoV钢寿命外推计算方法[J].热力发电, 2000(6):32-35.
【5】牛小驰,巩建鸣,姜勇, 等. 基于损伤力学的电厂主蒸汽管道蠕变损伤有限元分析[J].中国电机工程学报, 2008, 7(20):32-37.
【6】BECKER A A, HYDE T H, SUN W,et al. Benchmarks for finite element analysis of creep continuum damage mechanics [J].Computational Materials Science,2002,25(1/2):34-41.
【7】周顺深.用持久强度计算高温部件剩余寿命的不可靠性(下)[J].华东电力,1995(4):5-7.
【8】周顺深.用持久强度计算高温部件剩余寿命的不可靠性(上)[J].华东电力,1995(3):1-6.
【9】LARSON F R,MILLER J. A time-temperature relationship for rupture and creep stresses[J].Trans ASME,1952,74:765-775.
【10】古泉洁,朱小莎.火力发电厂锅炉的寿命诊断和管理[J].热力发电译丛,1986(1):43-45.
【11】耿鲁阳,刘建杰,巩建鸣,等.基于修正θ投影法炉管用Cr25Ni35Nb钢蠕变寿命预测[J].机械工程材料,2011,35(12):93-96.
【12】DYSON B F, GIBBONS T B. Tertiary creep in nickel-base superalloys:analysis of experimental data and theoretical synthesis[J].Acta Metallurgica,1987,35(9):2355-2369.
【13】常剑冰,许江晓.15CrMo1V主蒸汽管道焊缝在550 ℃运行温度下安全运行可靠性研究[R].郑州:河南电力试验研究所,2008.
【2】扬宜科, 吴天禄, 江先美, 等. 金属高温强度及试验[M].上海: 上海科学技术出版社, 1986.
【3】EVANS R W, WILSHIRE B. Creep of metals and alloys [M].US IMM North Americen Pub,1985.
【4】束国刚,李益民,赵彦芬, 等.基于蠕变曲线的12CrlMoV钢寿命外推计算方法[J].热力发电, 2000(6):32-35.
【5】牛小驰,巩建鸣,姜勇, 等. 基于损伤力学的电厂主蒸汽管道蠕变损伤有限元分析[J].中国电机工程学报, 2008, 7(20):32-37.
【6】BECKER A A, HYDE T H, SUN W,et al. Benchmarks for finite element analysis of creep continuum damage mechanics [J].Computational Materials Science,2002,25(1/2):34-41.
【7】周顺深.用持久强度计算高温部件剩余寿命的不可靠性(下)[J].华东电力,1995(4):5-7.
【8】周顺深.用持久强度计算高温部件剩余寿命的不可靠性(上)[J].华东电力,1995(3):1-6.
【9】LARSON F R,MILLER J. A time-temperature relationship for rupture and creep stresses[J].Trans ASME,1952,74:765-775.
【10】古泉洁,朱小莎.火力发电厂锅炉的寿命诊断和管理[J].热力发电译丛,1986(1):43-45.
【11】耿鲁阳,刘建杰,巩建鸣,等.基于修正θ投影法炉管用Cr25Ni35Nb钢蠕变寿命预测[J].机械工程材料,2011,35(12):93-96.
【12】DYSON B F, GIBBONS T B. Tertiary creep in nickel-base superalloys:analysis of experimental data and theoretical synthesis[J].Acta Metallurgica,1987,35(9):2355-2369.
【13】常剑冰,许江晓.15CrMo1V主蒸汽管道焊缝在550 ℃运行温度下安全运行可靠性研究[R].郑州:河南电力试验研究所,2008.
相关信息