Cause Analysis on Connection Dropout of Long Round Thread Casing
摘 要
某水平井发生接箍工厂端圆螺纹套管滑脱, 下部套管柱落井而未能打捞出。针对该起套管接头滑脱事故, 通过宏观分析、尺寸检测、螺纹参数测量、材料理化性能检验、实物试验、力学分析等方法对滑脱原因进行了分析。结果表明: 接箍紧密距参数不合格和套管抗粘扣性能差是套管接头发生脱扣失效的原因。
Abstract
A long round thread casing joint haven been pulled out from factory side of a coupling in a horizontal well, and the dropout casing string couldn′t got out of the well. Research on the dropout failure case was carried out. By means of macroscopic analysis, dimension measurement, thread parameters measurement, physical and chemical properties testing on the material, the full scale tests and mechanical analysis, the dropout cause was analyzed. The results showed that dropout failure was ascribed to the unqualified thread standoff of coupling and the poor thread sealant on anti galling performance.
中图分类号 TE931.2
所属栏目 质量控制与失效分析
基金项目 中国石油天然气集团公司科学研究与技术开发项目(2011A-4208)
收稿日期 2012/8/17
修改稿日期
网络出版日期
作者单位点击查看
备注潘志勇(1976-), 男, 工程师, 硕士。
引用该论文: PAN Zhi-yong,LIANG Ming-hua,ZHU Li-xia,XU Ting,SHEN Chen,TIAN Wei. Cause Analysis on Connection Dropout of Long Round Thread Casing[J]. Physical Testing and Chemical Analysis part A:Physical Testing, 2013, 49(5): 320~323
潘志勇,梁明华,朱丽霞,徐婷,沈沉,田伟. 长圆螺纹套管接头滑脱原因分析[J]. 理化检验-物理分册, 2013, 49(5): 320~323
被引情况:
【1】张钧,赵国仙,吕祥鸿,宋文文, "塔里木油田某井油管脱落原因分析",理化检验-物理分册 50, 845-848(2014)
【2】潘志勇,韩新利,王新虎,王建东,李东风,朱丽霞,刘心可, "某油井圆螺纹套管接头脱扣原因分析",理化检验-物理分册 51, 143-146(2015)
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】API Spec 5CTSpecification for Casing and Tubing[S].2011.
【2】API Spec 5BSpecification for Threading, Gauging, and Thread Inspection of Casing, Tubing, and Line Pipe Threads[S].2008.
【3】ISO 13679-2002Petroleum and Natural Gas Industries-Procedures for Testing Casing and Tubing Connections[S].
【4】ISO/TR 10400-2007Petroleum and Natural Gas Industries-Equations and Calculations for the Properties of Casing,Tubing,Drill Pipe and Line pipe Used as Casing or Tubing[S].
【5】SY/T 5322-2000套管柱强度设计方法[S].
【6】潘志勇, 燕铸, 刘文红, 等.两起套管脱扣失效的典型案例分析[J].钻采工艺, 2012, 35(5): 83-86.
【7】潘志勇, 陈鹏, 王建军, 等.某井偏梯形螺纹接头脱扣原因分析[J].金属热处理, 2012, 37(4): 124-127.
【8】潘志勇, 宋生印, 刘文红, 等.某井圆螺纹套管接头滑脱事故分析[J].石油矿场机械, 2011, 40(12): 20-24.
【9】吕拴录, 骆发前, 唐继平, 等.某井177. 8 mm套管固井事故原因分析[J].钻采工艺, 2009, 32(4): 98-101.
【10】宋治,冯耀荣.油井管与管柱技术及应用[M].北京:石油工业出版社,2007.
【11】吕拴录,韩勇,袁鹏斌,等.φ139.7 mm×7.72 mm J55长圆螺纹套管脱扣原因分析[J].钻采工艺,2005,28(2):73-77.
【12】高连新,史交齐,金烨.上扣扭矩对圆螺纹套管连接强度的影响[J].天然气工业,2005,25(2):87-89.
【13】齐俊林,罗维东,张宏,等.圆螺纹套管接头上扣与滑脱的数值模拟[J].石油大学学报(自然科学版),1998,24(4):68-71.
【2】API Spec 5BSpecification for Threading, Gauging, and Thread Inspection of Casing, Tubing, and Line Pipe Threads[S].2008.
【3】ISO 13679-2002Petroleum and Natural Gas Industries-Procedures for Testing Casing and Tubing Connections[S].
【4】ISO/TR 10400-2007Petroleum and Natural Gas Industries-Equations and Calculations for the Properties of Casing,Tubing,Drill Pipe and Line pipe Used as Casing or Tubing[S].
【5】SY/T 5322-2000套管柱强度设计方法[S].
【6】潘志勇, 燕铸, 刘文红, 等.两起套管脱扣失效的典型案例分析[J].钻采工艺, 2012, 35(5): 83-86.
【7】潘志勇, 陈鹏, 王建军, 等.某井偏梯形螺纹接头脱扣原因分析[J].金属热处理, 2012, 37(4): 124-127.
【8】潘志勇, 宋生印, 刘文红, 等.某井圆螺纹套管接头滑脱事故分析[J].石油矿场机械, 2011, 40(12): 20-24.
【9】吕拴录, 骆发前, 唐继平, 等.某井177. 8 mm套管固井事故原因分析[J].钻采工艺, 2009, 32(4): 98-101.
【10】宋治,冯耀荣.油井管与管柱技术及应用[M].北京:石油工业出版社,2007.
【11】吕拴录,韩勇,袁鹏斌,等.φ139.7 mm×7.72 mm J55长圆螺纹套管脱扣原因分析[J].钻采工艺,2005,28(2):73-77.
【12】高连新,史交齐,金烨.上扣扭矩对圆螺纹套管连接强度的影响[J].天然气工业,2005,25(2):87-89.
【13】齐俊林,罗维东,张宏,等.圆螺纹套管接头上扣与滑脱的数值模拟[J].石油大学学报(自然科学版),1998,24(4):68-71.
相关信息