旅大油田水源井处理系统腐蚀原因分析
          
Corrosion Analysis of Source Water Treatment System in Lv-da Offshore Oilfield

摘    要
渤海旅大油田三个采油平台的水源井水处理系统中LD10-1、LD5-2平台发生了严重的局部腐蚀,而LD4-2平台未发生腐蚀.通过对旅大油田各平台水源井水处理系统的水质、流速、腐蚀现状、腐蚀因素等对比分析,推断旅大油田水源井水处理系统管线的腐蚀是由于水流速较大,同时管线内部不平而导致的流体诱导局部腐蚀(FILC).根据分析结果,提出了解决方案.
标    签 采油平台   水源井水   流体诱导局部腐蚀   drilling and production platform   source water well   flow induced localized corrosion (FILC)  
 
Abstract
Lv-da(LD) offshore oilfield in Bohai bay has three drilling and production platforms which are LD10-1,LD5-2 and LD4-2.Severe localized corrosion occurred in source water system of LD5-2 and LD10-1 platforms;and no corrosion appeared in the system of LD4-2.From comparison and analysis of the water quality,flow rate,corrosion status,corrosive factor and corrosion product and so on,it is deduced that the reason of corrosion failure in LD offshore oilfield is FILC (flow induced localized corrosion) caused by high flow rate and accidented welding line in internal surface of pipeline.Some solution approaches against FILC are recommended.

中图分类号 TG172.5

 
  中国光学期刊网论文下载说明


所属栏目 应用技术

基金项目

收稿日期 2009/4/13

修改稿日期 2009/6/2

网络出版日期

作者单位点击查看


引用该论文: YAN Hua-yun,SU Chang-chun,ZHU Kai,WANG Lei,LIU Xuan-tao. Corrosion Analysis of Source Water Treatment System in Lv-da Offshore Oilfield[J]. Corrosion & Protection, 2010, 31(3): 242~244


论文评价
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
分享论文
分享到新浪微博 分享到腾讯微博 分享到人人网 分享到 Google Reader 分享到百度搜藏分享到Twitter

参考文献
【1】温斯顿里维 R.尤利格腐蚀手册(第2版)[M].北京:化学工业出版社,2005:168-174.
 
【2】Zhou X,Jepson W P.Corrosion in three-phase oil/water/gas slug flow in horizontal pipes[C]//NACE International,Corrosion/94,New Orleans LA:1994,Paper No.94026.
 
【3】Kang C,Wilkins R,Jepson W P.The effect of slug frequency on corrosion in high pressure inclined pipelines[C]//NACE International,Corrosion/96,Denver CO:1996,Paper No.96020.
 
【4】Schmitt G,Gudde T.Local mass transport coefficients and wall shear stresses at flow disturbances[C]//NACE International,Corrosion/95,P Orlando FL:1995,Paper No.95102.
 
【5】张智,施太和.井下油管的流动诱导腐蚀数值模拟研究[J].石油钻采工艺,2004(6):59-61.
 
相关信息
   标题 相关频次
 BZ25-1油田生产水处理系统SRB控制初探
 2
 FSM技术对海底管道中缓蚀剂应用效果的评价
 2
 GH4169镍基高温合金的高温低周疲劳损伤机理
 2
 HB4-49收紧螺母开裂原因
 2
 LF2铝合金燃油导管接头焊缝开裂原因及改进
 2
 Q235B钢热轧板带孔洞及边裂缺陷成因分析
 2
 Q460qNH高强度桥梁钢的耐蚀性能
 2
 T7951二次时效对7055铝合金疲劳裂纹扩展行为的影响
 2
 TC4钛合金表面污染层金相检验参数优选
 2
 X射线检测仿真软件成像的黑度修正
 2
 奥氏体不锈钢法兰开裂原因分析
 2
 奥氏体不锈钢管道腐蚀泄漏原因
 2
 标距对电工圆铜线拉力试验结果的影响
 2
 表面质量和缺口对Ti80合金弯曲性能的影响
 2
 不同表面状态对Ti80合金动态与静态力学性能的影响
 2
 不同冲击功对中碳合金钢腐蚀磨损的影响
 2
 不同方法测量截面积求铜合金圆导线电阻系数的不确定度评定
 2
 常减压装置换热器管箱腐蚀原因分析与防护措施
 2
 超声喷丸表面强化技术的研究现状与应用进展
 2
 臭氧在循环冷却水处理中的杀菌作用
 2
 镀锌钝化45A钢外套螺母及平管嘴腐蚀分析
 2
 二氧化碳驱注采井常用油套管钢的腐蚀行为
 2
 非晶纳米晶Ni-P合金的流动镀工艺
 2
 高铬铸铁组织与超声声速关系的测定
 2
 高速列车铜基粉末冶金闸片的制备及摩擦磨损性能
 2
 高效液相色谱法测定化妆品和洗涤剂中5种荧光增白剂的含量
 2
 高效液相色谱法测定蔬菜中19种氨基甲酸酯类农药的残留量
 2
 高效液相色谱法同时测定红景天药材中6种有效成分的含量及质量相关性分析
 2
 海上某油田生产井316L不锈钢毛细管泄漏失效分析
 2
 焊接材料及热输入对Q460钢厚板焊接接头拉伸性能的影响
 2