摘    要
在35 g·L-1NaCl水溶液中,用失重法、气体收集法和电化学方法研究了挤压变形对金属镁耐腐蚀性能的影响.结果表明:金属镁在挤压变形的过程中发生了动态再结晶,由大至几百微米大小不均匀的晶粒变为约25 μm的等轴晶,晶粒细化,晶界的面积增多,即阳极增多,阳极反应速率增加,耐腐蚀性能下降.
标    签 金属镁   晶粒细化   耐腐蚀性能   挤压变形   pure magnesium   grain refinements   corrosion resistance   extrusion deformation  
 
Abstract
Influence of extrusion deformation on the corrosion rate of pure magnesium was studied by means of weight loss,gas collection and electrochemical methods in 35 g·L-1 NaCl solution.The results show that the dynamic re-crystallization of pure magnesium occurres during the process of the extrusion deformation and the grain size is decreased from the size of a few hundreds micro meter (μm) to 25 μm.The area of grain boundaries as the anode is increased by the deformation.The reaction rate of the anode is much quicker than the magnesium without deformation and the corrosion resistance is decreased.

中图分类号 TG174.1

 
  中国光学期刊网论文下载说明


所属栏目

基金项目

收稿日期 2007/6/30

修改稿日期 2007/9/1

网络出版日期

作者单位点击查看

备注王赫男(1974-),女,辽宁沈阳人,讲师,硕士.

引用该论文: WANG He-nan,ZHAO Yu-hua,ZHANG Wei-xia. Influence of Extrusion Deformation on Corrosion Rate of Pure Magnesium[J]. Materials for mechancial engineering, 2008, 32(3): 42~44
王赫男,赵玉华,张伟霞. 挤压变形对金属镁耐腐蚀性能的影响[J]. 机械工程材料, 2008, 32(3): 42~44


被引情况:


【1】祁玉红,付巳超,高红,陈刚,陈旭, "AZ31镁合金板在PBS模拟体液中的腐蚀行为和拉伸性能",机械工程材料 38, 16-19(2014)



论文评价
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
分享论文
分享到新浪微博 分享到腾讯微博 分享到人人网 分享到 Google Reader 分享到百度搜藏分享到Twitter

参考文献
【1】张津.镁合金及应用[M].北京:化学工业出版社,2004:81.
 
【2】Achim Wendt,Knorad Weiss,Arye Ben-Dov,et al.Magnesium Castings in Aeronautics Applications-Special Requirements[C]//Magnesium Technology 2005.San Francisco,US:TMS (The Mineral,Metals & Materials Society),2005:269-273.
 
【3】Makar G L,Kruger J.Corrosion of Magnesium[J].International Materials Reviews,1993,38(2):138-153.
 
【4】Reidar Tunold,Hans Holtan,May-britt,et al.The corrosion of magnesium in aqueous solution containing chloride ions[J].Corrosion Science,1997,17:353-365.
 
【5】Greenbaltt J.A mechanism for the anodic dissolution of magnesium[J].Journal of the Electrochemistry Society,1956,103:539-547.
 
【6】Letzig D,Swiostek J,Bohlen J,et al.Magnesium Wrought Alloy Properties of the AZ-Series[C]//Magnesium Technology 2005.San Francisco,US:TMS (The Mineral,Metals & Materials Society),2005:55-59.
 
【7】Haitao Zhou,Chuming Liu,Qudong Wang,et al.Grain Refinement of Wrought AZ61 Magnesium Alloy[C]//Magnesium Technology 2005.San Francisco,US:TMS (The Mineral,Metals & Materials Society),2005:91-95.
 
【8】孙秋霞.材料腐蚀与防护[M].北京:冶金工业出版社,2003.
 
【9】Song G L,Atrens A,St John D.An Hydro-evolution Method for the Estimation of the Corrosion Rate of Magnesium alloys[C]//Magnesium Technology 2001.San Francisco,US:TMS (The Mineral,Metals & Materials Society),2001:255-259.
 
【10】Simaranov A Y,Sokolova I,Marshaknv A I,et al.Nature of the film on AZ91 magnesium alloy[J].Protection of Metal,1992,27:329-335.
 
相关信息
   标题 相关频次
 热挤压对铸态Mg-3.5Al-3.5Ca-0.6Mn合金组织与性能的影响
 3
 00Cr17Ni14Mo2钢法兰裂纹的产生原因
 2
 0Cr18Ni9Ti不锈钢表面渗锆合金层的耐腐蚀性能及抗高温氧化性能
 2
 1Cr17不锈钢表面TIG冷焊重熔和丝材熔敷工艺及改性层的组织和性能
 2
 1Cr18Ni9Ti不锈钢脉冲超窄间隙焊接头的组织及耐腐蚀性能
 2
 304不锈钢表面预处理对沉积CrMoN涂层性能的影响
 2
 316LN奥氏体不锈钢在含Cl-溶液中的腐蚀行为
 2
 316不锈钢表面等离子熔敷硼化物覆层的组织与性能
 2
 38CrMoAl钢表面不同厚度搪瓷涂层的组织和性能
 2
 3种成分中碳合金钢的显微组织及在含Cl-环境下的耐腐蚀性能
 2
 Al2O3掺杂与超声辅助对纯铝表面微弧氧化层结构与性能的影响
 2
 CT80钢级连续油管焊接接头在不同质量分数NaCl溶液中的电化学腐蚀行为
 2
 MnO含量对SJ612焊剂焊接18-8不锈钢接头组织和性能的影响
 2
 Mo2NiB2基金属陶瓷制备技术及应用的研究进展
 2
 Mo元素对货油舱下底板用船板钢耐腐蚀性能的影响
 2
 NixAlTiCrFeCoCu高熵合金的显微组织与性能
 2
 NiCrAlY合金粉添加量对超音速火焰喷涂WC-10Co4Cr涂层组织及性能的影响
 2
 NiTi形状记忆合金表面辉光离子氮化层的结构与性能
 2
 S355J2W耐候钢的耐腐蚀性能
 2
 TB8钛合金表面间歇式真空渗氮层的组织与性能
 2
 VC添加量对激光熔覆Fe50Mn30Cr10Co10高熵合金涂层组织和性能的影响
 2
 X80管线钢包埋渗铝层的显微组织和耐腐蚀性能
 2
 X80管线钢在库尔勒土壤模拟溶液中的腐蚀行为
 2
 X80管线钢在酸性土壤模拟溶液中的腐蚀行为
 2
 ZG45钢表面镍钴基熔覆层的显微组织与耐腐蚀性能
 2
 Zr-0.8Sn-0.35Nb-0.4Fe-0.1Cr-xBi合金在400 ℃过热蒸汽中的腐蚀行为
 2
 闭孔泡沫铝的表面积与耐腐蚀性能
 2
 表面形貌对1Cr11Ni2W2MoV不锈钢耐腐蚀性能的影响
 2
 薄带连铸B480GNQR耐候钢的腐蚀行为
 2
 不同表面处理对输电线路铁塔涂层性能的影响
 2