X80管线钢在延安地区水饱和土壤中的电化学腐蚀行为
          
Electrochemcial Corrosion Behavior of X80 Pipeline Steel in Yan′an Soil with Saturated Water

摘    要
采用电化学测试、扫描电镜及能谱仪分析等方法,研究了X80管线钢在延安地区水饱和土壤中的电化学腐蚀行为.结果表明:随腐蚀时间的延长,该钢的腐蚀速率先减小后增大,但腐蚀趋势增大,钢基体表面由以全面腐蚀为主转为以局部腐蚀为主,腐蚀机理为氧浓差腐蚀电池和局部腐蚀自催化效应,腐蚀速率主要受氧扩散过程控制;其腐蚀产物主要为铁的氧化物.
标    签 X80管线钢   电化学腐蚀行为   水饱和土壤   腐蚀机理   X80 pipeline steel   electrochemical corrosion behavior   soil with saturated water   corrosion mechanism  
 
Abstract
The electrochemical corrosion behavior of X80 pipeline steel was investigated in Yan′an soil with saturated water by using electrochemical measurement,scanning electron microscopy and energy dispersive spectrum analysis.The results show that the corrosion rate of the steel decreased first then increased with the prolongation of corrosion time,and the corrosion tendency increased.The corrosion morphology on the steel substrate was changed from uniform corrosion to localized corrosion.The corrosion mechanisms were oxygen-concentration corrosion cell and localized corrosion autocatalysis effect,and the corrosion rate was controlled by oxygen diffusion process.The corrosion product was main iron oxides.

中图分类号 TG172.7

 
  中国光学期刊网论文下载说明


所属栏目 材料性能及其应用

基金项目 陕西省教育厅专项科研计划项目

收稿日期 2009/9/28

修改稿日期 2010/6/25

网络出版日期

作者单位点击查看

备注李斌(1983-),女,甘肃兰州人,助理工程师.

引用该论文: LI Bin,ZHANG Yao-heng,XU Cong-min. Electrochemcial Corrosion Behavior of X80 Pipeline Steel in Yan′an Soil with Saturated Water[J]. Materials for mechancial engineering, 2010, 34(10): 65~67
李斌,张耀亨,胥聪敏. X80管线钢在延安地区水饱和土壤中的电化学腐蚀行为[J]. 机械工程材料, 2010, 34(10): 65~67


论文评价
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
分享论文
分享到新浪微博 分享到腾讯微博 分享到人人网 分享到 Google Reader 分享到百度搜藏分享到Twitter

参考文献
【1】曹楚南.中国材料的自然环境腐蚀[M].北京:化学工业出版社,2005:373-380.
 
【2】李晓刚,杜翠微,董超芳.X70钢的腐蚀行为与试验研究[M].北京:科学出版社,2006:1-20.
 
【3】胥聪敏,石凯.X80管线钢在格尔木土壤模拟溶液中的耐腐蚀性能[J].化工学报,2009,60(6):1513-1518.
 
【4】胥聪敏.X80管线钢在模拟盐碱土壤介质中的电化学腐蚀行为研究[J].材料工程,2009(9):66-70.
 
【5】胥聪敏,霍春勇,熊庆人,等.X80管线钢在酸性土壤模拟溶液中的腐蚀行为[J].机械工程材料,2009,33(5):29-32.
 
【6】胥聪敏.X80管线钢在库尔勒土壤环境中的电化学腐蚀行为研究[J].材料保护,2009,42(8):23-26.
 
【7】ZHOU Yun,XUE Xiao-huai,QIAN Bai-nian.Microstructure and property of coarse grain HAZ X80 pipeline steel[J].J Iron & Steel Res,Int,2005,12(6):54-58.
 
【8】冯耀荣,高惠临,霍春勇.管线钢显微组织的分析与鉴别[M].西安:陕西科学技术出版社,2008:236-286.
 
【9】费小丹,李明齐,许红梅,等.湿度对X70钢在卵石黄泥土中腐蚀行为影响的电化学研究[J].腐蚀科学与防护技术,2007,19(1):35-37.
 
【10】赵麦群,雷阿丽.金属的腐蚀与防护[M].北京:国防工业出版社,2004:133-141.
 
【11】杜翠薇,刘智勇,梁平.不同组织X70钢在库尔勒含饱和水土壤中的短期腐蚀行为[J].金属热处理,2008(6):15-19.
 
【12】HAMADOU L,KADRI A,BENBRAHIM N.Characterization of passive films formed on low carbon steel in borate buffer solution by electrochemical impedance spectroscopy[J].Applied Surface Science,2005,252(5):1510-1519.
 
【13】GARDINER C P,MELCHERS R E.Corrosion of mild steel in porous media[J].Corrosion Science,2002,44:2459-2478.
 
【14】曹楚南.腐蚀电化学原理[M].北京:化学工业出版社,1985:311.
 
相关信息
   标题 相关频次
 X80管线钢在西北盐渍土壤模拟溶液中的电化学腐蚀行为
 6
 0.8设计系数用X80管线钢焊接接头的失效评估曲线
 4
 X80管线钢在库尔勒土壤模拟溶液中的腐蚀行为
 4
 X80管线钢在水饱和碱性沙土中的腐蚀行为
 4
 X80管线钢在酸性土壤模拟溶液中的腐蚀行为
 4
 库尔勒土壤模拟溶液的pH对X80管线钢电化学腐蚀行为的影响
 4
 X80钢的CO2腐蚀电化学行为与机理研究
 3
 金属多孔材料腐蚀研究进展
 3
 1.4301不锈钢管线的腐蚀及修复
 2
 2A12铝合金微弧氧化陶瓷层的电化学腐蚀行为
 2
 304不锈钢表面磁控溅射制备Cr-C涂层的组织与耐高温电化学腐蚀性能
 2
 3A12、5052、6063铝合金在沿海大气环境中的腐蚀行为
 2
 B+M/A复相组织X80大变形管线钢的预应变脆化
 2
 Cl-对X80管线钢在HCO-3溶液中的电化学行为影响
 2
 CO2分压对X80管线钢腐蚀性能的影响
 2
 H2S分压对SM 80SS套管钢在CO2/H2S共存环境中高温高压腐蚀行为的影响
 2
 L320原油输送管道静置段的腐蚀机理
 2
 Q235钢在油田污水处理系统中的垢下腐蚀行为
 2
 QLT工艺热处理后X80管线钢的显微组织和力学性能
 2
 RTM成型技术在码头钢筋混凝土结构修复中的应用
 2
 SO42-对X80管线钢在酸性红壤模拟溶液中腐蚀行为的影响
 2
 SO2-4对X80管线钢在含Cl-的NaHCO3溶液中点蚀行为影响
 2
 SRB对油气管道腐蚀影响的研究进展
 2
 SS411NS型杀菌剂对Q235钢在循环冷却水中腐蚀行为的影响
 2
 WCp/2024Al基复合材料的腐蚀机理
 2
 X100管线钢在库尔勒土壤模拟溶液中的腐蚀行为
 2
 X65钢在CO2饱和油田水中的电化学行为和腐蚀机理
 2
 X80M管线钢热轧板卷取温度的优化
 2
 X80钢在新疆不同土壤环境中的氢脆行为
 2
 X80管线钢不同电化学充氢状态下的断裂特性
 2