Eddy Current Quantitative Test for Inner Defects of Heat-Exchange Tubes
摘 要
现阶段核电站换热管的内壁缺陷(内伤)的深度定量是通过检测信号的相位-缺陷深度的线性拟合曲线映射得到的。但根据现场数据分析的实际经验, 该种定量方法仍然存在偏差。结合实际内壁缺陷的涡流检测和金相解剖数据, 采用基于最小二乘的非线性拟合的方法制作新的相位和幅值标定曲线, 并采用统计方法比较现有拟合曲线与原始标定曲线下的定量数据准确性, 发现新拟合曲线下的定量结果更准确。
Abstract
The quantification of depth for inner defects of heat exchange tubes in nuclear power plant was realized by acquisition data mapped under the linear fitting of phase against defect depth curve. But according to practical experience of data analysis, there still exists deviation in this method. In this paper, based on eddy current and metallographic anatomy data, new phase and amplitude calibration curves were fitted by nonlinear least squares method, and then the comparison of data accuracy as analyzed by statistic method between fitting curves and the original one was undertaken and it was shown that the new phase fitting curves were more accurate for data quantification.
中图分类号 TG115.28 DOI 10.11973/wsjc201610014
所属栏目 试验研究
基金项目
收稿日期 2016/3/17
修改稿日期
网络出版日期
作者单位点击查看
联系人作者祁攀(qp928@163.com)
备注祁 攀(1982-), 男, 博士, 主要从事电磁无损检测相关技术研发。
引用该论文: QI Pan,WANG Bo,SHAO Wen-bin,CUI Hong-yan,YANG Chong-an,LIAO Shu-sheng. Eddy Current Quantitative Test for Inner Defects of Heat-Exchange Tubes[J]. Nondestructive Testing, 2016, 38(10): 60~63
祁 攀,王 波,邵文斌,崔洪岩,杨崇安,廖述圣. 换热管内壁缺陷涡流检测的定量方法[J]. 无损检测, 2016, 38(10): 60~63
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】丁训慎. 核电站蒸汽发生器传热管的降质及其无损检测技术[J]. 无损检测, 2008, 30(1): 30-33.
【2】ASME V-2004 锅炉及压力容器规范[S].
【3】JB/T 4730.6-2005 承压设备无损检测 第6部分:涡流检测[S].
【4】刘一舟, 曹刚, 王晓翔. 核电站钛管内壁缺陷判伤曲线[J]. 无损检测, 2010, 32(9): 719-721, 737.
【5】李柏年, 吴李斌. MATLAB数据分析方法[M]. 北京:机械工业出版社, 2011.
【6】谭荣波. SPSS统计分析实用教程[M].北京: 科学出版社, 2007.
【2】ASME V-2004 锅炉及压力容器规范[S].
【3】JB/T 4730.6-2005 承压设备无损检测 第6部分:涡流检测[S].
【4】刘一舟, 曹刚, 王晓翔. 核电站钛管内壁缺陷判伤曲线[J]. 无损检测, 2010, 32(9): 719-721, 737.
【5】李柏年, 吴李斌. MATLAB数据分析方法[M]. 北京:机械工业出版社, 2011.
【6】谭荣波. SPSS统计分析实用教程[M].北京: 科学出版社, 2007.
相关信息