Phased Array Ultrasonic Testing for Austenitic Stainless Steel Weld of Primary Coolant Piping in Nuclear Power Plant
摘 要
核电主管道采用离心铸造奥氏体不锈钢制造和焊接,其焊接质量直接关系到核反应堆的安全。目前核电主管道常采用窄间隙焊接技术,易产生侧壁未熔合缺陷,采用传统检测方法难以检出此类缺陷。采取理论分析、数值模拟以及超声相控阵检测、射线检测等多种手段相结合的方式,制定了核工程奥氏体不锈钢焊缝相控阵超声检测工艺,实现了相控阵超声检测方法在核电站主管道焊缝检测中的应用。
Abstract
Primary coolant piping in nuclear engineering are welded in centrifugally cast austenitic stainless steel (CCASS). The welding quality is directly related to the safety of nuclear reactors. Narrow gap welding is mostly used in CCASS, while lack of fusion in side walls appeared easily. Detecting it in common testing methods is difficult. The paper combined the theoretical research, analysis calculation, numerical simulation, phased array ultrasonic testing and radiographic testing. The tesing technique of CCASS is underlined and the technology has been applied to the primary coolant piping weld in nuclear engineering.
中图分类号 TG115.28 DOI 10.11973/wsjc201802006
所属栏目 试验研究
基金项目
收稿日期 2017/6/25
修改稿日期
网络出版日期
作者单位点击查看
备注严宇(1971-),男,本科,研究员级高工,主要从事无损检测工作
引用该论文: YAN Yu,ZHANG Xiaofeng,YANG Huimin,ZHOU Weilu. Phased Array Ultrasonic Testing for Austenitic Stainless Steel Weld of Primary Coolant Piping in Nuclear Power Plant[J]. Nondestructive Testing, 2018, 40(2): 24~28
严宇,张晓峰,杨会敏,周炜璐. 核电主管道奥氏体不锈钢焊缝的相控阵超声检测[J]. 无损检测, 2018, 40(2): 24~28
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】林莉,杨平华,张东辉,等. 厚壁铸造奥氏体不锈钢管道焊缝超声相控阵检测技术概述[J]. 机械工程学报,2012,48(4):12-20.
【2】李衍,冯兆国. 不锈钢焊缝的超声检测——现状与进展[J]. 无损探伤,2005,29(3):1-6.
【3】赵岁花,林莉,张东辉,等. 压水堆核电站主管道CCASS焊缝声学性能数值计算[J]. 无损探伤,2011,35(4):11-14.
【4】郑中兴. 奥氏体不锈钢焊缝的超声探伤方法[J]. 无损探伤,2005,29(4):12-16.
【5】晏荣明,李生田. 大厚度奥氏体焊缝超声波探伤的研究[J]. 无损探伤,1994,18(4):6-11.
【6】RAFAEL M,SYLVAIN V. On qualification of TOFD technique for austenitic stainless steel welds inspection[C]//9th ECNDT.Berlin:[s.n.],2006.
【7】CHEN Y B. Development of ultrasonic transducer testing austenitic stainless steel weld[C]//17th World Conference on Nondestructive Testing.Shanghai:[s.n.],2008.
【8】CORSEPIOS H W. 奥氏体焊缝的超声波检验[J]. 无损探伤,1996,20(2):26-33.
【9】顾炳忠. 奥氏体不锈钢焊缝的二维距离-波幅曲线检测方法[J]. 无损探伤,2010,34(7):551-552.
【10】王伟波. 奥氏体焊缝超声探伤用窄脉冲探头技术研究[D]. 哈尔滨:机械科学研究总院,2008.
【11】余菊生. 奥氏体不锈钢焊缝的超声波探伤[J]. 造船技术,1985(10):25-39.
【12】曹发美,吴爱军. 9%Ni钢球罐奥氏体焊缝超声波探伤[J]. 燕山油化,1992(1):6-48.
【13】康纪黔,李家鳌. 奥氏体不锈钢焊缝超声波检验规程[J]. 无损检测,2001,23(4):162-166.
【2】李衍,冯兆国. 不锈钢焊缝的超声检测——现状与进展[J]. 无损探伤,2005,29(3):1-6.
【3】赵岁花,林莉,张东辉,等. 压水堆核电站主管道CCASS焊缝声学性能数值计算[J]. 无损探伤,2011,35(4):11-14.
【4】郑中兴. 奥氏体不锈钢焊缝的超声探伤方法[J]. 无损探伤,2005,29(4):12-16.
【5】晏荣明,李生田. 大厚度奥氏体焊缝超声波探伤的研究[J]. 无损探伤,1994,18(4):6-11.
【6】RAFAEL M,SYLVAIN V. On qualification of TOFD technique for austenitic stainless steel welds inspection[C]//9th ECNDT.Berlin:[s.n.],2006.
【7】CHEN Y B. Development of ultrasonic transducer testing austenitic stainless steel weld[C]//17th World Conference on Nondestructive Testing.Shanghai:[s.n.],2008.
【8】CORSEPIOS H W. 奥氏体焊缝的超声波检验[J]. 无损探伤,1996,20(2):26-33.
【9】顾炳忠. 奥氏体不锈钢焊缝的二维距离-波幅曲线检测方法[J]. 无损探伤,2010,34(7):551-552.
【10】王伟波. 奥氏体焊缝超声探伤用窄脉冲探头技术研究[D]. 哈尔滨:机械科学研究总院,2008.
【11】余菊生. 奥氏体不锈钢焊缝的超声波探伤[J]. 造船技术,1985(10):25-39.
【12】曹发美,吴爱军. 9%Ni钢球罐奥氏体焊缝超声波探伤[J]. 燕山油化,1992(1):6-48.
【13】康纪黔,李家鳌. 奥氏体不锈钢焊缝超声波检验规程[J]. 无损检测,2001,23(4):162-166.
相关信息