Corrosion Monitoring of Grounding Net Based on Hollow Inflatable Seal Corrosion Unit
摘 要
提出并研制了一种基于预埋式指示单元的地网腐蚀状态监测装置:将中空充气密封状态的腐蚀单元连接在接地网上,与接地网导体一同埋入土壤发生同种腐蚀反应,当接地导体腐蚀深度等于腐蚀单元厚度时,腐蚀单元被蚀穿变成非密封状态,检测装置的密封性能可判断腐蚀单元的腐蚀状态。在实验室对研制的检测装置进行了可行性试验,并根据装置尺寸及参数建立对应的仿真模型。结果表明:该装置可明显反映腐蚀单元的腐蚀状态,且仿真结果与试验结果吻合度较好,该装置可实现免开挖接地网腐蚀状态的监测功能。
Abstract
A corrosion monitoring device for grounding net based on a pre-embedded indicator unit was proposed and developed. A corrosion unit with hollow inflatable sealed state was connected to the grounding net, and the same kind of corrosion reaction occurred when the grounding net conductor was also buried in the soil. When the corrosion depth of the grounding conductor was equal to the thickness of the corrosion unit, the corrosion unit was perforated by corrosion and became unsealed, and the corrosion state of the corrosion unit was judged by the sealing performance of the detection device. The feasibility test of the developed detection device was carried out in the laboratory, and the corresponding simulation model was established according to the device size and parameters. The results show that the device could clearly reflect the corrosion state of the corrosion unit, and the simulation results were in good agreement with the test results. The device can realize the function of monitoring the corrosion state of the grounding net without excavation.
中图分类号 TM83 DOI 10.11973/fsyfh-202005008
所属栏目 应用技术
基金项目 中国南方电网有限责任公司科技项目(SZKJXM20160188)
收稿日期 2018/9/17
修改稿日期
网络出版日期
作者单位点击查看
引用该论文: WANG Yazhou,ZHENG Zhihui,YAN Yuting,YIN Xiyu,TENG Yun,LU Hailiang. Corrosion Monitoring of Grounding Net Based on Hollow Inflatable Seal Corrosion Unit[J]. Corrosion & Protection, 2020, 41(5): 34
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】李谦. 电力系统接地网特性参数测量与应用[M]. 北京:中国电力出版社,2013.
【2】李景禄. 接地装置的运行与改造[M]. 北京:中国水利水电出版社,2005.
【3】吴向东. 500 kV输电线路接地网腐蚀分析及防护措施[J]. 腐蚀与防护,2002,23(12):545-547.
【4】钱之银,郁祖培. 直线型直流接地极腐蚀特性研究[J]. 高电压技术,1995,21(3):40-43.
【5】董晓辉,杨威,唐程,等. 特高压直流入地电流对附近杆塔地网腐蚀评估[J]. 高电压技术,2009,35(7):1546-1552.
【6】ZHANG B,ZHAO Z B,CUI X,et al. Diagnosis of breaks in substation's grounding grid by using the electromagnetic method[J]. IEEE Transactions on Magnetics,2002,38(2):473-476.
【7】刘洋,崔翔,赵志斌. 测量磁感应强度诊断变电站接地网断点[J]. 高电压技术,2008,34(7):1389-1394.
【8】张晓玲,陈先禄. 优化技术在发、变电所接地网故障诊断中的应用[J]. 高电压技术,2000,26(4):64-66.
【9】刘渝根,滕永禧,陈先禄,等. 接地网腐蚀的诊断方法研究[J]. 高电压技术,2004,30(6):19-21.
【10】何智强,文习山,潘卓洪,等. 一种地网腐蚀故障诊断的新算法[J]. 高电压技术,2007,33(4):83-86.
【11】黄文武,文习山,朱正国. 接地网腐蚀与断点诊断软件系统的开发[J]. 高电压技术,2005,31(7):42-44.
【12】张秀丽,骆平,莫逆,等. 接地网腐蚀状态电化学检测系统的开发与应用[J]. 中国电机工程学报,2008,28(19):152-156.
【13】MCINTOSH D H. Grounding where corrosion protection is required[J]. IEEE Transactions on Industry Applications,1982,IA-18(6):600-607.
【14】查全性. 电极过程动力学导论[M]. 北京:科学出版社,1976.
【15】DL/T 1554-2016接地网土壤腐蚀评价导则[S].
【16】谢苏江. 聚四氟乙烯的改性及应用[J]. 化工新型材料,2002,30(11):26-30.
【2】李景禄. 接地装置的运行与改造[M]. 北京:中国水利水电出版社,2005.
【3】吴向东. 500 kV输电线路接地网腐蚀分析及防护措施[J]. 腐蚀与防护,2002,23(12):545-547.
【4】钱之银,郁祖培. 直线型直流接地极腐蚀特性研究[J]. 高电压技术,1995,21(3):40-43.
【5】董晓辉,杨威,唐程,等. 特高压直流入地电流对附近杆塔地网腐蚀评估[J]. 高电压技术,2009,35(7):1546-1552.
【6】ZHANG B,ZHAO Z B,CUI X,et al. Diagnosis of breaks in substation's grounding grid by using the electromagnetic method[J]. IEEE Transactions on Magnetics,2002,38(2):473-476.
【7】刘洋,崔翔,赵志斌. 测量磁感应强度诊断变电站接地网断点[J]. 高电压技术,2008,34(7):1389-1394.
【8】张晓玲,陈先禄. 优化技术在发、变电所接地网故障诊断中的应用[J]. 高电压技术,2000,26(4):64-66.
【9】刘渝根,滕永禧,陈先禄,等. 接地网腐蚀的诊断方法研究[J]. 高电压技术,2004,30(6):19-21.
【10】何智强,文习山,潘卓洪,等. 一种地网腐蚀故障诊断的新算法[J]. 高电压技术,2007,33(4):83-86.
【11】黄文武,文习山,朱正国. 接地网腐蚀与断点诊断软件系统的开发[J]. 高电压技术,2005,31(7):42-44.
【12】张秀丽,骆平,莫逆,等. 接地网腐蚀状态电化学检测系统的开发与应用[J]. 中国电机工程学报,2008,28(19):152-156.
【13】MCINTOSH D H. Grounding where corrosion protection is required[J]. IEEE Transactions on Industry Applications,1982,IA-18(6):600-607.
【14】查全性. 电极过程动力学导论[M]. 北京:科学出版社,1976.
【15】DL/T 1554-2016接地网土壤腐蚀评价导则[S].
【16】谢苏江. 聚四氟乙烯的改性及应用[J]. 化工新型材料,2002,30(11):26-30.
相关信息