Analysis on common defects of magnetic particle detection in the switch rail manufacture
摘 要
道岔钢轨在制造加工过程中,由于原材钢轨、制造工艺及环境温度等因素的影响,易形成一些磁粉检测常见缺陷。分析这些常见缺陷的产生原因和磁痕显示特征,以为改进制造生产工艺防止缺陷的产生提供依据。
Abstract
In the process of manufacturing switch rail, as observed by magnetic particle testing, it is easy to form some common defects due to some influencing factors such as the steel raw material, manufacturing process and environmental temperature. The analysis on the causes of defects and magnetic image display characteristics shall be helpful for improving manufacturing process and providing basis for preventing the defect.
中图分类号 TG115.28 DOI 10.11973/wsjc202006015
所属栏目 实践研究
基金项目
收稿日期 2019/8/7
修改稿日期
网络出版日期
作者单位点击查看
备注朱欣欣(1990-),男,助理工程师,本科,主要从事道岔钢轨无损检测监督与检验工作
引用该论文: ZHU Xinxin. Analysis on common defects of magnetic particle detection in the switch rail manufacture[J]. Nondestructive Testing, 2020, 42(6): 68~69
朱欣欣. 道岔钢轨制造中磁粉检测的常见缺陷分析[J]. 无损检测, 2020, 42(6): 68~69
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】贺涛,陈晓渊,胡静. 超声探伤仪检定仪研制[J].声学技术, 2011, 30(4):199-203.
【2】周正干,李文涛,李洋,等.相控阵超声水浸C扫描自动检测系统的研制[J].机械工程学报,2017,53(12):28-34.
【3】贺涛,唐薇薇,刘夏茹.超声探伤仪检定装置数字化研究[J].中国测试,2014,40(4):111-114.
【4】孙景峰,刘慧英,舒蓉,等.可控超声探伤仪自动检定系统的研究与实现[J].机械科学与技术,2017,36(7):1085-1091.
【5】刘伟静,刘丹,韩强,等. 基于AD9910的70 MHz中频信号源设计[J]. 空间电子技术,2019,13:68-71.
【6】王硕,马永奎,高玉龙,等. 基于FPGA的改进结构的DDS设计与实现[J]. 电子技术应用,2016,42(3):28-34.
【7】王家敏,杨青慧,张怀武. 9 kHz~1.4 GHz高精度快速随机跳频DDS频率合成器[J]. 电子科技,2019,32(12):27-31.
【2】周正干,李文涛,李洋,等.相控阵超声水浸C扫描自动检测系统的研制[J].机械工程学报,2017,53(12):28-34.
【3】贺涛,唐薇薇,刘夏茹.超声探伤仪检定装置数字化研究[J].中国测试,2014,40(4):111-114.
【4】孙景峰,刘慧英,舒蓉,等.可控超声探伤仪自动检定系统的研究与实现[J].机械科学与技术,2017,36(7):1085-1091.
【5】刘伟静,刘丹,韩强,等. 基于AD9910的70 MHz中频信号源设计[J]. 空间电子技术,2019,13:68-71.
【6】王硕,马永奎,高玉龙,等. 基于FPGA的改进结构的DDS设计与实现[J]. 电子技术应用,2016,42(3):28-34.
【7】王家敏,杨青慧,张怀武. 9 kHz~1.4 GHz高精度快速随机跳频DDS频率合成器[J]. 电子科技,2019,32(12):27-31.
相关信息