The abnormal eddy current signal after stress relief heat treatment of U-tube
摘 要
U形传热管在制造过程中常采用电极加热的热处理方法对弯管段进行消应力热处理,热处理后需要使用内穿式探头对U形管进行涡流检测,信号分析时发现在电极夹钳位置,即热过渡区存在一个异常信号。通过多种无损检测方法的辅助检测,并采用整体再次固溶热处理的方式验证了该信号并不是缺陷信号,而是一种固有的工艺加工信号。
Abstract
During the manufacturing process of U-tube, the method of electrode heating heat treatment is often used to conduct stress-relieving heat treatment on the section of U-tube. After the heat treatment, the U-shaped pipe needs to be subjected to eddy current detection in the bend. During the signal analysis, it is found that there is an abnormal signal at the position of electrode clamp, that is, the thermal transition zone. It is verified that the signal is not due to a discontinuous signal, but is produced by an inherent processing signalas confimed by other non-destructive testing methods.
中图分类号 TG115.28 DOI 10.11973/wsjc202012012
所属栏目 试验研究
基金项目
收稿日期 2020/5/22
修改稿日期
网络出版日期
作者单位点击查看
联系人作者江华(380173845@qq.com)
备注江华(1985-),男,工程师,主要从事涡流及超声波无损检测工作
引用该论文: JIANG Hua,CAO Ping,YAN Shengzhi,LI Huanni,XIAO Qi,LI Weiyuan,XU Zhanbiao,MA Jun,PAN Huabiao. The abnormal eddy current signal after stress relief heat treatment of U-tube[J]. Nondestructive Testing, 2020, 42(12): 52~55
江华,曹萍,闫生志,李欢妮,肖琪,李伟源,徐占标,马骏,潘华彪. U形管弯管段消应力热处理过渡区的异常涡流信号[J]. 无损检测, 2020, 42(12): 52~55
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】陈丹, 赵岩,刘天佑.金属学与热处理[M].北京:北京理工大学出版社,2017.
【2】徐可北, 周俊华.涡流检测[M].北京:机械工业出版社,2004.
【3】郑晖, 林树青.超声检测[M].北京:中国劳动社会保障出版社,2008.
【4】胡赓祥, 蔡珣,戎咏华.材料科学基础[M].上海:上海交通大学出版社,2010.
【5】胡学之. 渗透检测[M].北京:中国劳动社会保障出版社,2008.
【2】徐可北, 周俊华.涡流检测[M].北京:机械工业出版社,2004.
【3】郑晖, 林树青.超声检测[M].北京:中国劳动社会保障出版社,2008.
【4】胡赓祥, 蔡珣,戎咏华.材料科学基础[M].上海:上海交通大学出版社,2010.
【5】胡学之. 渗透检测[M].北京:中国劳动社会保障出版社,2008.
相关信息