Automatic ultrasonic inspection of steel catenary riser welds
摘 要
在对钢悬链线立管(SCR)焊缝进行自动超声检测(AUT)的过程中,要求AUT具有可靠的检测能力和较高的检测精度。通过修正AUT缺陷评定方法,验证了AUT焊缝缺陷评定结果与金相检验结果的可靠性。结果表明,修正后的AUT评定结果与缺陷实际尺寸具有良好的一致性,为基于工程临界分析(ECA)验收标准的SCR管线的安装工程应用提供了借鉴。
Abstract
During automatic ultrasonic testing (AUT) of steel catenary riser (SCR) welds, it is required that the AUT technology should have reliable detection ability and high detection accuracy. The reliability of the AUT weld defect evaluation results and the metallographic examination results was verified by the modified AUT defect evaluation method. The results show that the modified AUT evaluation results are in good agreement with the actual size of the defect, which provides a reference for the installation engineering application of SCR pipeline based on the engineering critical analysis (ECA) acceptance standard.
中图分类号 TG115.28 DOI 10.11973/wsjc202107011
所属栏目 试验研究
基金项目 国家重点研发计划课题资助项目(2018YFC0310305)
收稿日期 2020/12/7
修改稿日期
网络出版日期
作者单位点击查看
备注陈亮(1983-),男,本科,高级工程师,主要从事海底管线检测工艺开发与应用工作
引用该论文: CHEN Liang,ZHANG Tianjiang,WU Yuan. Automatic ultrasonic inspection of steel catenary riser welds[J]. Nondestructive Testing, 2021, 43(7): 45~49
陈亮,张天江,吴员. 钢悬链线立管焊缝的自动超声检测[J]. 无损检测, 2021, 43(7): 45~49