Performance comparison of tubing in different injection wells
摘 要
采用盲孔法对不同注水井油管进行残余应力测试,用电化学腐蚀测试及水接触角法结合的方式对油管进行腐蚀性能测试,对不同材料的油管进行性能评价。结果表明:镀渗钨合金油管、普通油管、玻璃纤维增强塑料油管、防垢油管的残余应力依次由大到小;玻璃纤维增强塑料油管、镀渗钨合金油管、防垢油管、普通油管的抗腐蚀性能依次由大到小。
Abstract
The residual stress of different water injection tubings was tested by blind hole method, and the corrosion performance of tubings was tested by electrochemical corrosion test and water contact angle method, and the performance of tubings with different materials was evaluated. The results show that the residual stress of coated tungsten alloy tubing, ordinary tubing, fiber glass reinforced plastic tubing and anti-scaling tubing decreased in turn. The corrosion resistance of fiber glass reinforced plastic tubing, coated tungsten alloy tubing, anti scaling tubing, and ordinary tubing was from high to low.
中图分类号 TB304 TG115.5 DOI 10.11973/lhjy-wl202212009
所属栏目 试验技术与方法
基金项目
收稿日期 2022/5/20
修改稿日期
网络出版日期
作者单位点击查看
备注毕红军(1975-),男,高级工程师,主要从事油田注水等工作
引用该论文: BI Hongjun,XU Guoqiang,ZHU Yongqiang,QI Jiantao,SHI Xiuhui,BI Junhong,LI Chunlin. Performance comparison of tubing in different injection wells[J]. Physical Testing and Chemical Analysis part A:Physical Testing, 2022, 58(12): 39~42
毕红军,徐国强,朱永强,齐建涛,石秀慧,毕军红,李春林. 不同注水井油管性能对比[J]. 理化检验-物理分册, 2022, 58(12): 39~42
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】杨俊芬, 闫西峰,刘海锋.等.圆钢管加工方法诱导的残余应力分布检测与分析[J].工程力学,2017,34(9):202-210.
【2】YAN X F, YANG C. Experimental research and analysis on residual stress distribution of circular steel tubes with different processing techniques[J].Thin-Walled Structures,2019,144:1-12.
【3】杨晓,侯世忠,陈沛,等.常用的应力测试方法及其在船舶系统零部件中的应用[J].理化检验(物理分册),2020,56(4):18-22.
【4】BLÖDORN R, VIOTTI M R, SCHROETER R B, et al. Analysis of blind-holes applied in the hole-drilling method for residual stress measurements[J].Experimental Mechanics,2015,55(9):1745-1756.
【5】张雄,徐高鹏,熊健,等.残余应力无损检测点定位及实现方法[J].机械设计,2022,39(1):91-97.
【6】宋文涛.残余应力超声无损检测与调控技术研究[D].北京:北京理工大学,2016.
【7】XU C G, SONG W T, PAN Q X, et al. Nondestructive testing residual stress using ultrasonic critical refracted longitudinal wave[J].Physics Procedia,2015,70:594-598.
【8】梅振红.注水油管内防腐工艺技术研究[D].成都:西南石油大学,2014.
【9】ENCINAS-SÁNCHEZ V, DE MIGUEL M T, LASANTA M I, et al. Electrochemical impedance spectroscopy (EIS):an efficient technique for monitoring corrosion processes in molten salt environments in CSP applications[J].Solar Energy Materials and Solar Cells,2019,191:157-163.
【10】钱鸿昌,李海扬,张达威.超疏水表面技术在腐蚀防护领域中的研究进展[J].表面技术,2015,44(3):15-24,30.
【11】何石磊,毕宗岳,李周波,等.注水井用高抗挤套管的开发[J].焊管,2019,42(6):19-24.
【12】崔凯翔,田霖霖,赵磊,等.温度对X70钢在土壤中的早期腐蚀行为影响[J].延安大学学报(自然科学版),2021,40(4):93-97.
【2】YAN X F, YANG C. Experimental research and analysis on residual stress distribution of circular steel tubes with different processing techniques[J].Thin-Walled Structures,2019,144:1-12.
【3】杨晓,侯世忠,陈沛,等.常用的应力测试方法及其在船舶系统零部件中的应用[J].理化检验(物理分册),2020,56(4):18-22.
【4】BLÖDORN R, VIOTTI M R, SCHROETER R B, et al. Analysis of blind-holes applied in the hole-drilling method for residual stress measurements[J].Experimental Mechanics,2015,55(9):1745-1756.
【5】张雄,徐高鹏,熊健,等.残余应力无损检测点定位及实现方法[J].机械设计,2022,39(1):91-97.
【6】宋文涛.残余应力超声无损检测与调控技术研究[D].北京:北京理工大学,2016.
【7】XU C G, SONG W T, PAN Q X, et al. Nondestructive testing residual stress using ultrasonic critical refracted longitudinal wave[J].Physics Procedia,2015,70:594-598.
【8】梅振红.注水油管内防腐工艺技术研究[D].成都:西南石油大学,2014.
【9】ENCINAS-SÁNCHEZ V, DE MIGUEL M T, LASANTA M I, et al. Electrochemical impedance spectroscopy (EIS):an efficient technique for monitoring corrosion processes in molten salt environments in CSP applications[J].Solar Energy Materials and Solar Cells,2019,191:157-163.
【10】钱鸿昌,李海扬,张达威.超疏水表面技术在腐蚀防护领域中的研究进展[J].表面技术,2015,44(3):15-24,30.
【11】何石磊,毕宗岳,李周波,等.注水井用高抗挤套管的开发[J].焊管,2019,42(6):19-24.
【12】崔凯翔,田霖霖,赵磊,等.温度对X70钢在土壤中的早期腐蚀行为影响[J].延安大学学报(自然科学版),2021,40(4):93-97.
相关信息