Comparative analysis of fluorescent penetrant testing with different system sensitivity
摘 要
使用不同系统灵敏度的荧光渗透液对人工盲孔缺陷试样进行检测,分析验证了在不同系统灵敏度的荧光渗透液下人工盲孔缺陷显示结果的差异。结果表明,采用相同系统灵敏度的荧光渗透液对人工盲孔进行检测时,后乳化型较水洗型灵敏度更高。对于孔洞类缺陷而言,直径和深度的关系是影响渗透检测灵敏度的重要因素。
Abstract
The artificial blind hole defect samples were tested by using fluorescent penetrants with different system sensitivities, and the differences in the display results of artificial blind hole defects by using fluorescent penetrants with different system sensitivities were analyzed and verified. The results show that the sensitivity of the post-emulsification penetrant is higher than that of the water washable penetrant when the fluorescent penetrants with the same system sensitivity are used to detect the artificial blind hole. For holes, the relation between their diameter and depth is an important factor affecting the sensitivity of penetrant testing.
中图分类号 TG115.28 DOI 10.11973/wsjc202301008
所属栏目 试验研究
基金项目
收稿日期 2022/5/28
修改稿日期
网络出版日期
作者单位点击查看
备注王树志(1980-),男,主要从事渗透检测,磁粉检测等无损检测技术研究工作
引用该论文: WANG Shuzhi,XIAO Xionghui,LIU Guanghua,GAO Wenbo,CAO Heming,BAI Yi. Comparative analysis of fluorescent penetrant testing with different system sensitivity[J]. Nondestructive Testing, 2023, 45(1): 39~42
王树志,肖雄晖,刘广华,高文博,曹合明,白铱. 不同系统灵敏度荧光渗透检测的对比分析[J]. 无损检测, 2023, 45(1): 39~42
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】赵新宝,刘林,张卫国,等.单晶高温合金晶体取向的研究进展[J].材料导报,2007,21(10):62-66.
【2】蔡祖鹏,陈玉华,黄永德.镍基单晶高温合金凝固组织特征的研究进展[J].材料导报,2013,27(19):86-89.
【3】赵乃仁,李金国,刘金来,等.籽晶法生长高温合金单晶凝固界面研究[J].材料工程,2007,35(11):24-27.
【4】赵新宝,刘林,杨初斌,等.镍基单晶高温合金凝固缺陷研究进展[J].材料工程,2012,40(1):93-98.
【2】蔡祖鹏,陈玉华,黄永德.镍基单晶高温合金凝固组织特征的研究进展[J].材料导报,2013,27(19):86-89.
【3】赵乃仁,李金国,刘金来,等.籽晶法生长高温合金单晶凝固界面研究[J].材料工程,2007,35(11):24-27.
【4】赵新宝,刘林,杨初斌,等.镍基单晶高温合金凝固缺陷研究进展[J].材料工程,2012,40(1):93-98.
相关信息