酸性油气田用高性能不锈钢的选材与应用
          
Materials Selection and Application of High Performance Stainless Steels Used in Sour Oil and Gas Fields

摘    要
分析了酸性油气田选材标准及体系, 重点综述了酸性油气工业用高性能不锈钢的选材特点、评价方法标准和用材现状, 还对常用材料性价比进行了简单分析。
标    签 酸性油气田   不锈钢   耐腐蚀   应力腐蚀   选材   sour oil and gas field   stainless steel   corrosion resistance   stress corrosion   materials selection  
 
Abstract
The selection standards and system of metallic materials used in sour oil and gas industries are analyzed, and the emphasis is focused on metallic materials selection characteristics, evaluation standards, utilized status of high performance stainless steels for sour oil and gas fields. In addition, the cost of material selection is analyzed briefly.

中图分类号 TG174.22 TG133.4

 
  中国光学期刊网论文下载说明


所属栏目 专论

基金项目 重庆市科技攻关计划(CSTC2009AB4082; CSTC2010AA4054)项目; 中国机械工业集团有限公司科技发展基金(SINOMACH09科242号)项目

收稿日期 2010/11/23

修改稿日期 2011/1/13

网络出版日期

作者单位点击查看


备注刘海定, 工程师,

引用该论文: LIU Hai-ding,WANG Dong-zhe,WEI Han-dong,ZHANG Yu-bi,DUAN Min-jiang,CHEN Deng-hua. Materials Selection and Application of High Performance Stainless Steels Used in Sour Oil and Gas Fields[J]. Corrosion & Protection, 2011, 32(10): 817


论文评价
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
分享论文
分享到新浪微博 分享到腾讯微博 分享到人人网 分享到 Google Reader 分享到百度搜藏分享到Twitter

参考文献
【1】魏星, 郭建春, 赵金洲, 等. 中国油气资源现状及发展建议[J]. 中外能源, 2008, 13(5):17-22.
 
【2】韩大匡. 中国油气田开发现状、面临的挑战和技术发展方向[J]. 中国工程科学, 2010, 12(5):51-57.
 
【3】岑芳, 李治平, 赖枫鹏, 等. 高含硫气田开发难点及对策[J]. 现代地质, 2007, 21(增刊):63-65.
 
【4】王正东. 各国由酸性气体生产硫磺产量概况和酸性气田开采中的一些问题[J]. 石油与天然气化工, 1980(4):38-48.
 
【5】张忠铧, 张春霞, 陈长风. 高温高压H2S腐蚀试验方法的国际标准分析[J]. 世界钢铁, 2007(4):17-21.
 
【6】葛有琰, 杜强. 含硫化氢环境油气田开发材质选择标准方法——NACE MR 0175/IS0 15156的应用概要[J]. 石油与天然气化工, 2008, 37(5):410-415.
 
【7】NACE MR0175/ISO 15156-2:2003(E). Petroleum and natural gas industries-materials for use in H2S-containing environments in oil and gas production-Part 2:Cracking-resistant carbon and low alloy steels, and the use of cast irons[S].
 
【8】M B Kermani, D Harrop. Experimental limit of Sour Service for Tubular Steels[C]//NACE Corrosion/91, Houston:11-15.
 
【9】Kovach C W, Redmerski L S. Corrosion resistance of high-performance stainless in cooling water and other refinery environments[C]//NACE Corrosion/84, New Orleans:2-6.
 
【10】Arnvig P E, Wasielewska W. Stress corrosion behaviour of highly alloyed stainless steels under severe evaporative conditions[J]. ACOM(Avesta Sheffield AB), 1993(3).
 
【11】NACE MR0175/ISO 15156-3:2003(E). Petroleum and natural gas industries-materials for use in H2S-containing environments in oil and gas production-Part 3:Cracking-resistant CRAs (corrosion resistant alloys) and other alloys[S].
 
【12】Bauernfeind D, Mori G. Corrosion of superaustenitic stainless steels in chloride-and sulfate-containing media-influence of alloying elements Cr, Mo, N, and Cu[C]//NACE Corrosion/2003, Houston:16-20.
 
【13】Nicole Kinsman, Gary Carinci, Jim Feritz. 双相不锈钢新钢种、应用和标准概述[C]//第三届中国国际双相不锈钢大会, 山西太原:2009.
 
【14】Bahri Ozturk, John F Grubb. Review of N08367 seawater service experience[C]//NACE Corrosion/2005, Houston:18-20.
 
相关信息
   标题 相关频次
 铁镍基合金925在含硫、H2S和CO2盐溶液中的腐蚀行为
 8
 一种新型国产高性能耐蚀合金在湿H2S环境中的应力腐蚀性能
 6
 316L不锈钢人孔盖板爆裂原因分析
 4
 从失效案例探讨不锈钢的应力腐蚀问题
 4
 大型高炉煤气重力除尘波纹管的失效分析
 4
 高压换热器U形管管口开裂分析
 4
 含H2S环境中马氏体不锈钢的应力腐蚀敏感性
 4
 某石化电厂脱硫装置导流罩失效分析
 4
 304不锈钢表面锈蚀原因分析
 3
 316LN奥氏体不锈钢在含Cl-溶液中的腐蚀行为
 3
 表面形貌对1Cr11Ni2W2MoV不锈钢耐腐蚀性能的影响
 3
 不锈钢环保型彩色工艺及其耐腐蚀性能
 3
 不锈钢在不同介质中的正负交变电脉冲处理及其对耐腐蚀性的影响
 3
 加工工艺对不锈钢直螺纹接头耐蚀性的影响
 3
 模拟油气田环境下抗硫管的腐蚀行为对比
 3
 液氢槽车不锈钢管道开裂失效分析
 3
 1Cr13不锈钢在湿H2S环境中的应力腐蚀行为
 2
 1Cr5Mo钢弯管开裂原因分析
 2
 201型不锈钢在酸性食物模拟环境中的腐蚀行为
 2
 20CrMnTi齿轮钢的应力腐蚀行为
 2
 2205双相钢临界点蚀温度测量方法的比较
 2
 22Cr双相不锈钢与304L、316L钢在氯化物溶液中耐应力腐蚀性能的比较
 2
 303Cu不锈钢在拉拔及机加工时开裂原因
 2
 304、316不锈钢和Inconel 617镍基合金在硝酸熔盐中的腐蚀行为
 2
 304L不锈钢换热管泄漏原因分析
 2
 304L不锈钢疏水管焊接接头的腐蚀疲劳行为
 2
 304不锈钢大小头短期内开裂原因分析
 2
 304不锈钢点腐蚀的声发射检测
 2
 304不锈钢焊缝的相控阵超声检测
 2
 304不锈钢焊管应力腐蚀开裂原因
 2