Galvanic Corrosion of Seawater Cooling Pipe Lined Copolymers
摘 要
采用海水浸泡、电偶腐蚀、模拟腐蚀和扫描电镜分析等方法, 研究了脱氧铜(TUP)紫铜冷却水管内壁内衬共聚物后的电偶腐蚀性能。结果表明, 内衬乙烯-丙烯酸共聚物(EAA)或涂敷环氧玻璃鳞片后, TUP紫铜管与高电位金属连接引起的电偶腐蚀能够得到有效抑制, 内衬EAA的性能优于涂敷环氧玻璃鳞片。
Abstract
Galvanic corrosion of copper cooling pipes lined with copolymer were tested by seawater immersed test, galvanic corrosion test, simulated pipe test and scanning electron microscopy. The results showed that the galvanic corrosion between red copper and high potential metal was efficiently controlled by lining ethylene acrylic ocid (EAA) copolymer or overlaying epoxy glass flakes, the effect of lining ethylene acrylic acid (EAA) copolymer was more excellent than that of overlaying epoxy glass-flakes.
中图分类号 TG174
所属栏目 试验研究
基金项目
收稿日期 2013/4/26
修改稿日期
网络出版日期
作者单位点击查看
备注杨青松,工程师,硕士,
引用该论文: YANG Qing-song,ZHANG Bo,DONG Cai-chang,HAN Dong-rui. Galvanic Corrosion of Seawater Cooling Pipe Lined Copolymers[J]. Corrosion & Protection, 2013, 34(7): 583
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】王曰义. 海水冷却系统的腐蚀及其控制[M]. 北京:化学工业出版社,2006,56-59.
【2】尹建平,谢礼波. 舰船长效防腐保护涂层[J]. 环境技术,2001,18(6):39-41.
【3】孙胜, 赵三元, 柏永清, 等. 涂塑钢管常用的塑料粉末涂料[J]. 钢管,2000,29(1):58-60.
【4】陈仁慈,周宝茂. 塑覆铜水管的制造技术[J]. 化学建材,2006,22(5):22-23.
【2】尹建平,谢礼波. 舰船长效防腐保护涂层[J]. 环境技术,2001,18(6):39-41.
【3】孙胜, 赵三元, 柏永清, 等. 涂塑钢管常用的塑料粉末涂料[J]. 钢管,2000,29(1):58-60.
【4】陈仁慈,周宝茂. 塑覆铜水管的制造技术[J]. 化学建材,2006,22(5):22-23.
相关信息