高钢级大口径焊管残余应力的测试方法
          
Test Methods for Residual Stress in Large-diameter Welded Pipe of High Grade Steel

摘    要
针对X80钢大口径UOE,JCOE和SAWH(螺旋缝埋弧焊)三种焊管,研究了盲孔法、切块法和切环法在高钢级大口径焊管残余应力测试中的应用。结果表明:对于这三种管型,通过切环法估算的残余应力与盲孔法和切块法的测试值较为接近,三种方法的结果重合性较好。
标    签 大口径焊管   残余应力   测试方法   盲孔法   切块法   切环法   测点布置   large-diameter welded pipe   residual stress   test method   blind hole method   slab method   cutting ring method   test point arrangement  
 
Abstract
For three kinds of large-diameter welded pipe of X80 steel including UOE, JCOE and SAWH (helical submerged arc welding) pipe, applications of the blind hole method, slabmethod, cutting ring methodin residual stress testing for large-diameter welde dpipe of high grade steel were studied. The results showed that, for the three kinds of pipe, the estimate results of residual stress by cutting ring method were close to the test values by blind hole method and slab method, the results of three methods coincided better.

中图分类号 TG404

 
  中国光学期刊网论文下载说明


所属栏目

基金项目

收稿日期 2010/10/12

修改稿日期

网络出版日期

作者单位点击查看

备注熊庆人(1969-),女,高级工程师,博士。

引用该论文: XIONG Qing-ren,LI Xiao,XU Cong-min,LI Jian,ZHANG Wei-wei,WEI Zun-yi. Test Methods for Residual Stress in Large-diameter Welded Pipe of High Grade Steel[J]. Physical Testing and Chemical Analysis part A:Physical Testing, 2011, 47(5): 265~269
熊庆人,李霄,胥聪敏,李健,张伟卫,卫遵义. 高钢级大口径焊管残余应力的测试方法[J]. 理化检验-物理分册, 2011, 47(5): 265~269


论文评价
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
分享论文
分享到新浪微博 分享到腾讯微博 分享到人人网 分享到 Google Reader 分享到百度搜藏分享到Twitter

参考文献
【1】罗金恒,郑茂盛,熊庆人,等.螺旋缝埋弧焊管残余应力的评价方法[J].压力容器,2008,25(3):7-14.
 
【2】XIONGQing-ren, FENG Yao-rong, HUO Chun-yong, et al. Themeasurement and control of residual stress in spiral sub-merged arc welded pipe[C]//Proceedings of IPC′ 02, 4th International Pipeline Conference. Calgry, Alberta, Canada: [s.n.],2002.
 
【3】吉玲康,颜峰,霍春勇,等.螺旋缝埋弧焊管的水压和稳压试验及残余应力[J].石油机械,2000,28(3):15-19.
 
【4】VLACLAV Linhart,JANA Sigmundoval, VLADIS-LAV Ochodek. Some comparisons of residual stress measurements on pressurized pipes by the holed drilling and magnetoelastic methods[J]. Electronics folyoirat, 2008(1):34-37.
 
【5】月兰.焊管的残余应力测试与研究[J].实验力学, 2001,16(3):305-312.
 
【6】LAWA M, PRASK H, LUZIN V, et al. Residual stress measurements in coil, linepipe and girth welded pipe[J].Materials Science and Engineering A, 2006, 437:60-63.
 
【7】颜峰,吉玲康,冯耀荣.油气输送焊管残余应力测试方法的研究[J].石油机械,1999,27(4):18-20.
 
【8】CB3395-1992 残余应力测量方法钻孔应变释放法[S].
 
【9】ASTM E837-08e1 Standard Test Method for Determining Residual Stresses by the Hole-drilling Straingage Method[S].
 
【10】XIONG Qing-ren, ZHAO Wen-zhen, ZHENG Mao-sheng, et al. Effects of axial and radial distortion on residual stress of HSAW pipe[C]//2009 ASME Pressure Vessels and Piping Conference. Prague:[s. n.], 2009.
 
相关信息
   标题 相关频次
 X80钢大口径螺旋焊管的残余应力
 8
 成型过程对焊管残余应力的影响
 6
 螺旋缝埋弧焊管残余应力的测试与控制
 6
 切环法和盲孔法测试大口径厚壁X80钢级埋弧焊管的残余应力
 5
 X80管线钢在库尔勒土壤模拟溶液中的腐蚀行为
 4
 X80管线钢在酸性土壤模拟溶液中的腐蚀行为
 4
 基于分段冷压法7050大型铝合金锻件残余应力的消减
 4
 某循环流化床锅炉TP347H钢再热器管的开裂原因
 4
 热时效对消除钢结构焊接残余应力的工艺评估
 4
 影响高级别管线钢拉伸强度测试的因素
 4
 7050和7075铝合金板材的淬火残余应力
 3
 残余应力的超声检测方法
 3
 测定钢板残余应力的改进盲孔法
 3
 大功率柴油机气缸盖的残余应力
 3
 压路机压轮焊接变形和残余应力的有限元模拟
 3
 0.8设计系数用X80管线钢焊接接头的失效评估曲线
 2
 16MnD5钢板焊接件热影响区开裂原因分析
 2
 16MnR钢板焊接对接接头残余应力磁记忆检测研究
 2
 16Mn钢弯管的开裂原因
 2
 17Cr2Ni2Mo钢的表面复合喷丸强化
 2
 18Cr2Ni4WA钢氮化和喷丸强化处理的残余应力及性能
 2
 1Cr18Ni9Ti不锈钢导管开裂原因分析
 2
 2A14铝合金去应力热时效的作用
 2
 300M钢热损伤的巴克豪森检测
 2
 304不锈钢薄壁焊管表面残余拉应力的测定及消除
 2
 304不锈钢焊缝附近的点蚀损伤发展规律
 2
 304不锈钢焊管应力腐蚀开裂原因
 2
 30CrMnSiNi2A钢轮轴表面镀硬铬区域开裂的原因及控制措施
 2
 316L奥氏体不锈钢碱液储罐开裂原因
 2
 316L不锈钢板式换热器泄漏原因
 2