Microstructure and Cutting Properties of Two kinds of TiC-based Cermets
摘 要
采用纳米TiN加入微米TiC混合粉末(A)和纳米TiC0.7N0.3固溶体粉末(B)两种配料,用无压烧结方法制备了A和B两种金属陶瓷材料及其相应刀具,对材料的组织和刀具的切削性能进行了研究.结果表明: A陶瓷相由黑色的芯和灰色的壳构成;而B陶瓷相兼有黑白两种芯和灰色的壳结构.分布于陶瓷相晶界处的纳米颗粒具有增强陶瓷基体的作用.在相同切削条件下,刀具A的切削性能比刀具B更好;高速切削时,氧化和扩散磨损加速了刀具的失效进程.
Abstract
Two kinds of cermets (cermet A and B) and their cutters (Tool A and B),were sintered by TiC micronpowders with TiN nanoparticles and TiC0.7N0.3solution nanopowders under pressureless condition.The study of microstructures and cutting tests showed that ceramic phases of A had black cores surrounded by grey rims,while B exhibited black and white cores with grey rims.TiN nanoparticles distributed among ceramic grainboundaries can improve strength of ceramic matrix.Tool A behaved higher cutting performances in comparison with Tool B at the same cutting conditions.Oxidation and diffusion wears accelerated failing progress of cermet cutters at higher cutting speeds.
中图分类号 TG135
所属栏目
基金项目
收稿日期 2005/11/7
修改稿日期 2006/8/24
网络出版日期
作者单位点击查看
备注韩成良(1978-),男,安徽合肥人,讲师,硕士.
引用该论文: HAN Cheng-liang,GUAN Hang-min,GAO Da-ming,HU Kun-hong,LIU Ning. Microstructure and Cutting Properties of Two kinds of TiC-based Cermets[J]. Materials for mechancial engineering, 2006, 30(11): 21~24
韩成良,管航敏,高大明,胡坤宏,刘宁. 两种TiC基金属陶瓷的组织结构与刀具切削性能[J]. 机械工程材料, 2006, 30(11): 21~24
被引情况:
【1】戴鸿霞,熊惟皓,张国鹏,陈肖, "TaC含量对Ti(C,N)基金属陶瓷抗热震性能的影响",机械工程材料 36, 10-13(2012)
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】王文光.金属陶瓷刀具的新进展[J].工具技术,1995,29(10):36-37.
【2】现代机夹可转位刀具实用手册编委会.现代机夹可转位刀具实用手册[M].北京:机械工业出版社,1994.
【3】孙丽虹,张希顺,田杰谟,等.Si3N4基微米/纳米陶瓷微观组织[J].稀有金属,1999,23(4):193-197.
【4】Stearns L C,Zhao J,Harmmar M P.Processing and microstructure development in Al2O3-SiC nanocomposites [J].J Euro Ceram Soc,1992,10(6):473-477.
【5】黄传真,张蕾,孙高祚,等.ZrO2/(W,Ti)C陶瓷材料摩擦磨损性能[J].机械工程材料,2005,29(5):41-44.
【6】Ahn Sun-Yong,Kang Shinhoo.Formation of core/rim structures in Ti(C,N)-WC-Ni cermets via a dissolution and precipitation process[J].J Am Ceram Soc,2000,(6):1489-1494.
【7】刘宁,黄新民,周杰,等.Ti(C,N)基金属陶瓷中陶瓷相芯/壳组织的观察与分析[J].硅酸盐学报,2000,28(4):381-384.
【8】孙德明,刘立红,许崇海,等.Al2O3/Cr3C2/(W,Ti)C陶瓷抗弯强度的研究[J].机械工程材料,2005,29(8):43-45.
【9】徐智谋,易新建,熊惟皓,等.纳米TiC增强Ti(C,N)基金属陶瓷材料的组织与性能研究[J].功能材料,2003,36(6):396-398.
【10】何 林,黄传真,刘玉先,等.Ti(C,N)基金属陶瓷的力学性能与显微结构的研究[J].硅酸盐学报,2003,31(3):324-328.
【11】高家化,沈志坚,丁子上.陶瓷基纳米复合材料[J].复合材料学报,1994,11(1):1-7.
【12】肖诗纲.现代刀具材料[M].重庆:重庆大学出版社,1992.129-130.
【13】Frederic Monteverde,Alida Bellosi.Oxidation behavior of titanium carbonitride based materials[J].Corrosion Science,2002,44:1967-1982.
【2】现代机夹可转位刀具实用手册编委会.现代机夹可转位刀具实用手册[M].北京:机械工业出版社,1994.
【3】孙丽虹,张希顺,田杰谟,等.Si3N4基微米/纳米陶瓷微观组织[J].稀有金属,1999,23(4):193-197.
【4】Stearns L C,Zhao J,Harmmar M P.Processing and microstructure development in Al2O3-SiC nanocomposites [J].J Euro Ceram Soc,1992,10(6):473-477.
【5】黄传真,张蕾,孙高祚,等.ZrO2/(W,Ti)C陶瓷材料摩擦磨损性能[J].机械工程材料,2005,29(5):41-44.
【6】Ahn Sun-Yong,Kang Shinhoo.Formation of core/rim structures in Ti(C,N)-WC-Ni cermets via a dissolution and precipitation process[J].J Am Ceram Soc,2000,(6):1489-1494.
【7】刘宁,黄新民,周杰,等.Ti(C,N)基金属陶瓷中陶瓷相芯/壳组织的观察与分析[J].硅酸盐学报,2000,28(4):381-384.
【8】孙德明,刘立红,许崇海,等.Al2O3/Cr3C2/(W,Ti)C陶瓷抗弯强度的研究[J].机械工程材料,2005,29(8):43-45.
【9】徐智谋,易新建,熊惟皓,等.纳米TiC增强Ti(C,N)基金属陶瓷材料的组织与性能研究[J].功能材料,2003,36(6):396-398.
【10】何 林,黄传真,刘玉先,等.Ti(C,N)基金属陶瓷的力学性能与显微结构的研究[J].硅酸盐学报,2003,31(3):324-328.
【11】高家化,沈志坚,丁子上.陶瓷基纳米复合材料[J].复合材料学报,1994,11(1):1-7.
【12】肖诗纲.现代刀具材料[M].重庆:重庆大学出版社,1992.129-130.
【13】Frederic Monteverde,Alida Bellosi.Oxidation behavior of titanium carbonitride based materials[J].Corrosion Science,2002,44:1967-1982.
相关信息