ANALYSIS OF BROKEN REASON OF THE HOLLOW WATER-COOLING WIRE IN THE GENERATOR UNIT STATOR
摘 要
借助扫描电子显微镜、光学显微镜和力学性能测试等分析手段对发电机定子线棒空心水冷断裂导线的断口、金相组织和力学性能进行了分析。结果表明,水冷导线是由于制造时未将水冷导线捆扎紧,造成线捆松动,在微动力的摩擦作用下,产生疲劳断裂。
Abstract
The fracture surface and the microstructure and the mechanical properties of the hollow water-cooling wire in the generator unit stator were studied by scanning electron microscope (SEM) and optical microscope and tensile testing. The result showed that the hollow water-cooling wire was fatigue fracture,which caused by friction because of loosed hollow water-cooling wire.
中图分类号 TM311
所属栏目 质量控制与失效分析
基金项目
收稿日期 2006/9/22
修改稿日期
网络出版日期
作者单位点击查看
备注李朝晖(1965-),男,工程师,学士。
引用该论文: LI Zhao-hui,GAI Xiu-ying,SUN Ji-hong,GUAN Xue-ming. ANALYSIS OF BROKEN REASON OF THE HOLLOW WATER-COOLING WIRE IN THE GENERATOR UNIT STATOR[J]. Physical Testing and Chemical Analysis part A:Physical Testing, 2007, 43(9): 480~482
李朝晖,盖秀颖,孙继红,关学铭. 发电机定子线棒空心水冷导线断裂原因分析[J]. 理化检验-物理分册, 2007, 43(9): 480~482
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】GB/T 5231-2001 加工铜及铜合金化学成分和产品形状[S].
【2】GB/T 1527-1997 铜及铜合金拉制管[S].
【3】GB/T 6394-2002 金属平均晶粒度测定方法[S].
【2】GB/T 1527-1997 铜及铜合金拉制管[S].
【3】GB/T 6394-2002 金属平均晶粒度测定方法[S].
相关信息