Numerical Simulation of Erosion in Elbow Based on CFD and Optimization of Thickness Measurement
摘 要
弯头作为改变介质流向的管件, 冲蚀是其失效的主要原因。应用计算流体动力学CFD软件对弯头的冲蚀过程进行了模拟仿真, 通过分析仿真结果提出了弯头测厚布点的优化方案。现场的检测结果表明: 优化后的布点方案能够全面掌握弯头外弧面的冲蚀情况, 避免了漏检的发生。
Abstract
The role of elbow is to change the flow of medium. The failure of elbow is mainly due to erosion. The numerical simulation of the erosion process about four direction of medium in elbow and horizontal elbow is established by using CFX. The optimization of thickness measurement is based on the simulation analysis outcomes. The on-site testing results show that the optimized method can get full grasp of the erosion status of outer surface of elbow. The undetected errors are avoided effectively.
中图分类号 TG115.28 DOI 10.11973/wsjc201608008
所属栏目 试验研究
基金项目
收稿日期 2015/12/17
修改稿日期
网络出版日期
作者单位点击查看
备注廖飞龙(1988-), 男, 助理工程师, 主要从事特种设备及钻机的检验工作。
引用该论文: LIAO Fei-long,LIU Jiong,ZHOU Yong-lin,ZHAO Xiao,WAN Fu,ZHOU Zhao-ming. Numerical Simulation of Erosion in Elbow Based on CFD and Optimization of Thickness Measurement[J]. Nondestructive Testing, 2016, 38(8): 34~37
廖飞龙,刘 炯,周咏琳,赵 潇,万 夫,周兆明. 基于CFD软件的管道弯头冲蚀数值模拟及弯头测厚布点优化[J]. 无损检测, 2016, 38(8): 34~37
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】魏秀芝. 气力输送颗粒在输送管弯头中的运动及磨损[J].黑龙江石油化工,1996(2):36-39.
【2】高福庆. 管道检测的必要性[J].管道技术与设备, 1998(1):40-42.
【3】郎需庆, 赵志勇, 宫宏, 等.油气管道事故统计分析与安全运行对策[J].安全、健康和环境, 2006,6(10): 15-17.
【4】曾涌捷.天然气管道弯头冲蚀失效机理研究[J].石油与化工设备,2011,14(2):44-46.
【5】李明高, 李明.ANSYS 13.0流场分析技术及应用实例[M]. 北京: 机械工业出版社, 2012:349.
【6】谢龙汉, 赵新宇, 张炯明.ANSYS CFX流体分析及仿真[M].北京: 电子工业出版社, 2012:152-157.
【2】高福庆. 管道检测的必要性[J].管道技术与设备, 1998(1):40-42.
【3】郎需庆, 赵志勇, 宫宏, 等.油气管道事故统计分析与安全运行对策[J].安全、健康和环境, 2006,6(10): 15-17.
【4】曾涌捷.天然气管道弯头冲蚀失效机理研究[J].石油与化工设备,2011,14(2):44-46.
【5】李明高, 李明.ANSYS 13.0流场分析技术及应用实例[M]. 北京: 机械工业出版社, 2012:349.
【6】谢龙汉, 赵新宇, 张炯明.ANSYS CFX流体分析及仿真[M].北京: 电子工业出版社, 2012:152-157.
相关信息