摘 要
对玻璃模具钢LN17进行了化学成分设计,采用EAF+LF+VOD+ESR冶炼、锻造和预硬化工艺进行生产,分析了其组织与性能。结果表明:LN17钢预硬化后,硬度偏差 ≤ 2 HRC,组织为均匀的回火索氏体组织及少量残余奥氏体,综合力学性能较14Cr17Ni2钢的有很大提高。
Abstract
The chemical composition of glass die steel LN17 was designed. The process of EAF+LF+VOD+ESR smelting, forging and pre-hardening was used to produce the steel. The microstructure and properties of the steel were analyzed. The results showed that LN17 steel pre-hardening, hardness deviation less than 2 HRC and the organization for the uniform sorbite microstructure and residual austenite of 14Cr17Ni2 steel, a comprehensive mechanical performance has greatly improved.
中图分类号 TG142.45
所属栏目
基金项目
收稿日期
修改稿日期
网络出版日期
作者单位点击查看
备注汝亚彬(1981-),高级工程师,学士,从事模具材料研发
引用该论文: RU Yabin,LIU Baoshi,KANG Aijun,LIU Wei,CAO Lihong,MU Lifeng,YU Dan,SHEN Lin. Development of Pre-Hardening Die Steel LN17 for Glass[J]. Materials for mechancial engineering, 2017, 41(Z2): 44~46
汝亚彬,刘宝石,刘玮,曹丽红,于宗洋,谭凯,唐亮,于海鹏. FS2738预硬化塑料模具钢大型模块的组织和性能[J]. 机械工程材料, 2017, 41(Z2): 44~46
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】刘晴,邵文宝,吴春京. 玻璃模具材料选择的研究进展[J]. 锻造技术,2005,26(6):551-554.
【2】徐进,陈再枝. 模具钢[M]. 北京:冶金工业出版社,2002:22~24.
【3】崔忠圻. 金属学与热处理[M]. 北京:机械工业出版社,2000:298.
【2】徐进,陈再枝. 模具钢[M]. 北京:冶金工业出版社,2002:22~24.
【3】崔忠圻. 金属学与热处理[M]. 北京:机械工业出版社,2000:298.
相关信息