Recognition of Defect Signals for Phased Array Ultrasonic Inspection of Small-Diameter Tubes
摘 要
针对锅炉小径管的部分常见典型缺陷,结合理论仿真与实际检测数据的比对,总结出不同类型缺陷的典型特征。结果可作为缺陷识别的指导方法,方便检测人员更加准确地进行缺陷定性评价。
Abstract
In view of some common typical defects of small-diameter boiler tubes and based on the comparison of theoretical simulation and actual testing data, the typical characteristics of different types of defects are summarized and refined in this paper. Obtained results can be used as a guidance for defect identification, and they are beneficial for the inspectors to qualitatively evaluate the defect more accurately.
中图分类号 TG115.28 DOI 10.11973/wsjc201905006
所属栏目 试验研究
基金项目
收稿日期 2018/10/18
修改稿日期
网络出版日期
作者单位点击查看
联系人作者刘叙笔(liuxubi@163.com)
备注刘叙笔(1980-),男,高级工程师,主要从事电站金属材料无损检测工作
引用该论文: LIU Xubi,MA Junpeng,LÜ,Bo,YUE Xianqiang. Recognition of Defect Signals for Phased Array Ultrasonic Inspection of Small-Diameter Tubes[J]. Nondestructive Testing, 2019, 41(5): 22~27
刘叙笔,马君鹏,吕博,岳贤强. 小径管相控阵超声检测的缺陷信号识别方法[J]. 无损检测, 2019, 41(5): 22~27
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】路宝学,张健.小径管环焊缝的相控阵超声检测[J].机械工程师,2018(8):55-56,60.
【2】刘长福, 蔡文河, 郭德瑞, 等. 承压设备中、小径管管座角焊缝的超声检测[J]. 无损检测, 2018, 40(8):28-33, 38.
【3】侯金刚, 杨齐, 潘强华, 等. 小径管对接接头相控阵超声检测关键工艺参数选择[J]. 中国特种设备安全, 2018, 34(7):36-40.
【4】贾石,纪海波,王占富.超声导波检测技术在小径管检测中的应用[J].锅炉制造,2018(4):49-51.
【5】张瑞, 田旭海, 王海生, 等. 薄壁不锈钢小径管的失效分析及相控阵检测[J]. 无损检测, 2018, 40(6):28-31.
【6】杨克强. 小径管焊接接头射线检测[J]. 科技风, 2018(3):143.
【2】刘长福, 蔡文河, 郭德瑞, 等. 承压设备中、小径管管座角焊缝的超声检测[J]. 无损检测, 2018, 40(8):28-33, 38.
【3】侯金刚, 杨齐, 潘强华, 等. 小径管对接接头相控阵超声检测关键工艺参数选择[J]. 中国特种设备安全, 2018, 34(7):36-40.
【4】贾石,纪海波,王占富.超声导波检测技术在小径管检测中的应用[J].锅炉制造,2018(4):49-51.
【5】张瑞, 田旭海, 王海生, 等. 薄壁不锈钢小径管的失效分析及相控阵检测[J]. 无损检测, 2018, 40(6):28-31.
【6】杨克强. 小径管焊接接头射线检测[J]. 科技风, 2018(3):143.
相关信息