A new method for testing elongation after fracture of steel wire rope
摘 要
通过对钢索的产品技术要求、钢索组成结构、试样夹持方式、试验参数等方面进行分析,提出了一种钢索钢丝绳断后伸长率测试的新方法。试验结果表明:采用新试验工艺、专用工装及大量程引伸计进行断后伸长率测试,不仅能够锁紧试样,而且又不损伤试样,拉伸过程符合GB/T 228.1—2010的要求。该方法填补了实验室的检测空白,获得了可靠的试验数据,满足了产品使用部门的测试需求。
Abstract
Based on the analysis of the technical requirements and composition structure of the steel wire rope, the clamping method of the sample and the test parameters, a new method for testing elongation after fracture of steel wire rope was proposed. The test results show that the new test process, special tooling and a large range extensometer were used to test the elongation after fracture, which not only could lock the sample, but also did not damage the sample. The tensile process met the standard requirements of GB/T 228.1-2010. The method filled the testing gap in the laboratory, obtained reliable test data, and met the test requirements of the product use department.
中图分类号 TG115.5+2 DOI 10.11973/lhjy-wl202209006
所属栏目 试验技术与方法
基金项目
收稿日期 2022/1/19
修改稿日期
网络出版日期
作者单位点击查看
备注于湃(1980-),男,工程师,主要从事金属材料力学性能检测分析工作
引用该论文: YU Pai,LIU Tianzhao,LIU Junbo,WANG Lin,WU Li,SUN Qi. A new method for testing elongation after fracture of steel wire rope[J]. Physical Testing and Chemical Analysis part A:Physical Testing, 2022, 58(9): 23~26
于湃,刘天钊,刘俊博,王林,吴莉,孙奇. 钢索钢丝绳断后伸长率测试新方法[J]. 理化检验-物理分册, 2022, 58(9): 23~26
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
相关信息