Gas well casing damage dectection based on phased array ultrasonic technology
摘 要
采用超声波套损检测仪器,对气井套管进行检测,并对检测结果进行评价。结果表明,采用数据列结合先进算法的可视化图谱全局扫描分析能对套管损坏情况进行有效评估,可以对典型井段的腐蚀损伤进行定量和定性,有望为管柱力学的完整性和安全性评估提供参考。
Abstract
The ultrasonic casing damage detection instrument was used to detect the casing of the gas well, and the detection results were evaluated. The results show that the data series combined with the visual map global scanning analysis of the advanced algorithm can effectively evaluate the casing damage, and can quantitatively and qualitatively determine the corrosion damage of typical well sections, which is expected to be used for the integrity and safety evaluation of the pipe string mechanics for reference.
中图分类号 TG115.28 DOI 10.11973/wsjc202210013
所属栏目 试验研究
基金项目
收稿日期 2021/12/1
修改稿日期
网络出版日期
作者单位点击查看
备注曹志峰(1981-),男,硕士,高级工程师,主要从事特种设备检验检测相关研究工作
引用该论文: CAO Zhifeng,TONG Qiyun,BAI Haiqing. Gas well casing damage dectection based on phased array ultrasonic technology[J]. Nondestructive Testing, 2022, 44(10): 57~59
曹志峰,仝其云,白海青. 基于相控超声技术的气井套管损伤检测[J]. 无损检测, 2022, 44(10): 57~59
共有人对该论文发表了看法,其中:
人认为该论文很差
人认为该论文较差
人认为该论文一般
人认为该论文较好
人认为该论文很好
参考文献
【1】王向阳, 韩金良, 刘建伟, 等.超声波套损检测技术在煤层气井套管检测中的应用[J].中国科技论文, 2021, 16(9):1030-1034.
【2】邵青, 黄森清, 肖华, 等.威远页岩气井套管变形失效检测及对策[J].内蒙古石油化工, 2021, 47(3):52-54.
【3】路远涛, 朱立江, 马铭悦, 等.深层气注产井高压密闭测井工艺及应用[J].石油管材与仪器, 2017, 3(3):54-58.
【4】许立志, 王明灼, 曾黄麟.CNG储气井套管检测技术综述[J].四川理工学院学报(自然科学版), 2009, 22(6):111-115.
【5】黄华, 徐菲, 罗庆, 等.油气井套管变形段位置及其缺陷的涡流检测[J].无损检测, 2020, 42(10):40-48.
【6】何海峰, 罗宇昆, 涂斌, 等.自适应灰狼小波去噪法在变压器套管引线超声检测中的应用[J].无损检测, 2020, 42(3):54-59.
【2】邵青, 黄森清, 肖华, 等.威远页岩气井套管变形失效检测及对策[J].内蒙古石油化工, 2021, 47(3):52-54.
【3】路远涛, 朱立江, 马铭悦, 等.深层气注产井高压密闭测井工艺及应用[J].石油管材与仪器, 2017, 3(3):54-58.
【4】许立志, 王明灼, 曾黄麟.CNG储气井套管检测技术综述[J].四川理工学院学报(自然科学版), 2009, 22(6):111-115.
【5】黄华, 徐菲, 罗庆, 等.油气井套管变形段位置及其缺陷的涡流检测[J].无损检测, 2020, 42(10):40-48.
【6】何海峰, 罗宇昆, 涂斌, 等.自适应灰狼小波去噪法在变压器套管引线超声检测中的应用[J].无损检测, 2020, 42(3):54-59.
相关信息