    CAO Gang, LIU Xiang-Mei. Eddy Current Testing of Through-Hole of a Heat Exchanger Tube[J]. Nondestructive Testing, 2009, 31(8): 619-621.
    Citation: CAO Gang, LIU Xiang-Mei. Eddy Current Testing of Through-Hole of a Heat Exchanger Tube[J]. Nondestructive Testing, 2009, 31(8): 619-621.

    Eddy Current Testing of Through-Hole of a Heat Exchanger Tube

    More Information
    • Received Date: August 25, 2008
    • Eddy current testing standards at home and abroad are usually provided for through-hole defects in the signal phase for about 40 °. However, the actual detection of heat exchanger tube was found that the phase signal of leakage defects was as large as about 105 °, and as small as near 25 °. If the conventional phase-depth curve was used to evaluate the defect depth, the error would be very serious. The laws of signal phase of through-hole in relevant literature and the actual testing were analyzed, and it was found that through-hole defect signal phase was related to aperture size and wall thickness and such as volume factors. The more amount metal loss, the smaller the phase; and on the contrary, the less amount the metal loss, the larger the phase. So when testing the pipe defect with eddy current method, signal amplitude and phase should be combined to evaluate the defect size.
    • [1]
      ASME锅炉及压力容器委员会无损检测分委员会.ASME锅炉及压力容器规范国际性规范: 第Ⅴ卷 无损检测 第8章 管材制品的涡流检测(2004版)[M].中国《ASME规范产品》协作网(CACI),译.北京: 中国石化出版社,2004.
      [2]
      JB/T 4730.6—2005 承压设备无损检测 第6部分: 涡流检测[S].
      [3]
      美国无损检测学会.美国无损检测手册·电磁卷[M].《美国无损检测手册》译审委员会,译.上海: 世界图书出版公司,1999.
      [4]
      《国防科技工业无损检测人员资格鉴定与认证培训教材》编审委员会.涡流检测[M].北京: 机械工业出版社,2004.
      [5]
      杨宝初.传热管涡流信号研究[J].无损检测,1998,20(5): 132.

    Catalog

      Article views (3) PDF downloads (1) Cited by()

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return